"One of the problems with bucket glazes is convincing people to be certain that they'…"

Norm Stuart replied Jan 6, 2014 to glaze cracks and peels off the pot

5 Jan 12, 2014
Reply by Celia Walker

"Gerstley Borate makes a good substitute for man-made frits. The resulting clear tend…"

Norm Stuart replied Dec 30, 2013 to Clear cone 6 recipe

7 Dec 30, 2013
Reply by Norm Stuart

"Revitalizing plaster molds - Not that I know of. If you're using Sodium Silicate as…"

Norm Stuart replied Dec 29, 2013 to Re-vitalizing old plaster molds

1 Dec 29, 2013
Reply by Norm Stuart

"Looking at the Pink Panther glaze ingredients, the only potential toxic ingredient i…"

Norm Stuart replied Dec 18, 2013 to Insight-Live Glaze Database Training

6 Oct 8, 2014
Reply by Darthe Hues

"The hotter your kiln is the more vibrant the color you'll see radiating through the…"

Norm Stuart replied Nov 30, 2013 to Issues firing Duncan Teacher Plus Kiln to Cone 6

4 Dec 1, 2013
Reply by Brent Farler

"If you're trying to equalize temperature in a bisque, or give glaze enough time to r…"

Norm Stuart replied Nov 13, 2013 to hold cycle

11 Nov 13, 2013
Reply by Norm Stuart

"Once you find yourself frequently baby-sitting your kiln-sitter at the end of each f…"

Norm Stuart replied Nov 9, 2013 to hold cycle

11 Nov 13, 2013
Reply by Norm Stuart

"Digitalfire reports, "A down side to boron in certain glazes is that it combines wit…"

Norm Stuart replied Nov 7, 2013 to Clear cone 6 recipe

7 Dec 30, 2013
Reply by Norm Stuart

"Since the recipe uses just 8% Ferro Frit 4193, you can substitute Ferro Frit 3124 wh…"

Norm Stuart replied Nov 7, 2013 to jan wallace dry glaze recipe - frit question

1 Nov 7, 2013
Reply by Norm Stuart

"Knowing what is in your raw materials is important to glaze chemistry as well as foo…"

Norm Stuart replied Oct 29, 2013 to Food Safe Glazes

5 Oct 29, 2013
Reply by Norm Stuart

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service