"Thanks for the tip norm. I have suspected that regular bentonite changed some of my…"

Chantay Poulsen replied May 15, 2014 to Bentone-EW

1 May 15, 2014
Reply by Chantay Poulsen

"Go online and find the operating Manuel for your kiln. It will answer a lot of your…"

Chantay Poulsen replied May 15, 2014 to New Kiln, Newbie Potter

8 May 30, 2014
Reply by Nadine Mercader

"Another use is to use it as a teaching tool. It clearly explains the effects of incr…"

Chantay Poulsen replied May 15, 2014 to Can one predict the appearance of a glaze? (part II: tri-axial graphs of the Flux, Glass-formers and Amfoteres)

5 May 17, 2014
Reply by Daniel Spruyt

"Thanks for the info Norm. Will try and read tonight. That Peacock looks good. The Ga…"

Chantay Poulsen replied May 6, 2014 to Dave's Blue

9 May 6, 2014
Reply by Chantay Poulsen

"Here is the corner of a platter in Stadards Red rock, cone 6, I glazed in the Dave's…"

Chantay Poulsen replied May 5, 2014 to Dave's Blue

9 May 6, 2014
Reply by Chantay Poulsen

"Thanks, I had been taught this at a glaze class but for got.  I have my test batch m…"

Chantay Poulsen replied May 1, 2014 to Dave's Blue

9 May 6, 2014
Reply by Chantay Poulsen

"Thanks Nadine,  I have done this before but for some reason couldn't get it to work…"

Chantay Poulsen replied Apr 30, 2014 to Dave's Blue

9 May 6, 2014
Reply by Chantay Poulsen

"Mala, I just saw something like this.  It was using a used 20 ft. shipping container…"

Chantay Poulsen replied Apr 25, 2014 to Beyond the Market Tent to a Rolling Showroom

7 Jun 9, 2018
Reply by josi rica

"Im just making samples right now so I will try it with the custer.  The original gla…"

Chantay Poulsen replied Apr 21, 2014 to Feldspar Question

3 Apr 21, 2014
Reply by Chantay Poulsen

"OK, I just thought to look on US Pigments website and there it is.  So, yes, G-200 i…"

Chantay Poulsen replied Apr 21, 2014 to Feldspar Question

3 Apr 21, 2014
Reply by Chantay Poulsen

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service