I've found Bentone-EW has incredible suspending power compared with VeeGum or bentonite. And best of all it doesn't lump together in cold water as bentonite does.

After reading about Bentone-EW on John Tilton's blog, I bought a pound from Trinity Ceramics in Texas.  Sayed Abbas at US Pigment says he will soon be carrying this product as well.    http://www.tiltonpottery.com/life_cycle.php

http://trinityceramic.com/     http://www.uspigment.com/chemicals.shtml

The Bentone-EW manufacturer says this type of bentonite is "highly beneficiated" which is usually a code-word for subjecting their raw bentonite to some sort of chemical processing after it is mined.  The suspending power is 15 times that of ordinary bentonite.

Manufacturers PDF Information Sheet     Digitalfire page on Bentone-EW

Ferro Frit makes CM-941, a beautiful but problematic ^06 all-in-on leaded cadmium sulfide frit.  Add 2% bentonite to suspend this frit and it fires into a bubbly black mess.  In the past I've had to "suspend" this frit with 4% xanthan gum.

So instead of using 2% VeeGum bentonite, I successfully suspended this all-frit glaze using 0.2% Bentone-EW.

As you can see in the photo below, the miniscule 0.2% of Bentone-EW does affect the color somewhat, but at least it's still red rather than foamy matte black.

Trinity Ceramic Supply says Bentone-EW "is not a big seller", which I can easily understand. A single pound of Bentone-EW is sufficient to suspend at least 500 pounds of all-frit glaze.

Views: 580

▶ Reply to This

Replies to This Discussion

Thanks for the tip norm. I have suspected that regular bentonite changed some of my gazes. Next time I mix new batches I will test.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service