"Gold glazes, to the best of my knowledge, all have very high percentages of manganes…"

Norm Stuart replied Sep 8, 2014 to looking for a nice gold-ish glaze

4 Nov 19, 2014
Reply by Judy Smith

"Tom - Tin-Chrome colorants are probably the most particular about the type of base g…"

Norm Stuart replied Sep 5, 2014 to Cone 6 tests with Digital Fire Bases

6 Apr 25, 2015
Reply by Norm Stuart

"Your peak kiln temperature, and the duration of that peak temperature, determines wh…"

Norm Stuart replied Aug 22, 2014 to Iron Reds

9 Aug 22, 2014
Reply by Brent Farler

"Pete's Tomato Red #13 certainly needs something when made with Laguna Red Iron Oxide…"

Norm Stuart replied Aug 21, 2014 to Iron Reds

9 Aug 22, 2014
Reply by Brent Farler

"Don't refire Amaco Seaweed or slow-cool it after a ^6 firing.  The green waves runni…"

Norm Stuart replied Aug 6, 2014 to Amaco potter's choice

18 Apr 9, 2015
Reply by Norm Stuart

"That's a pretty good list, and here's my suggestions for you: 1.)  drop Darvan 7, a…"

Norm Stuart replied Aug 4, 2014 to Talc versions at Aardvark

7 Aug 4, 2014
Reply by Darthe Hues

"Most Amaco glazes are pudding thick to keep the ingredients fully suspended, so they…"

Norm Stuart replied Aug 4, 2014 to Amaco High Fire Glazes

13 Aug 7, 2014
Reply by Marti Howell

"I've found that the New Amaco Firebrick Red makes a great base glaze to layer other…"

Norm Stuart replied Aug 3, 2014 to Amaco High Fire Glazes

13 Aug 7, 2014
Reply by Marti Howell

"Thanks George.  A thin layer of slip made of the clay you're on top of the Kyanite r…"

Norm Stuart replied Jul 29, 2014 to Repairing a bisque ware.

4 Jul 29, 2014
Reply by Norm Stuart

"Matte glazes have a irregular microscopic surface like sandpaper which scatter the l…"

Norm Stuart replied Jul 29, 2014 to Recipe of Reliable matt (very) yellow cone 6 glaze

25 Jun 16, 2015
Reply by Harold Roberts

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service