Hi all, I'm a newbie, but have been working with an awesome potter.  She has developed a glaze used around the lip of pots.  It leaves a wonderful runny gold-ish over all her glazes.  Anyone seen any glazes like this or have recipes?

Views: 5342

▶ Reply to This

Replies to This Discussion

Gold glazes, to the best of my knowledge, all have very high percentages of manganese dioxide with small amounts of iron. Most of these recipes become extremely fluid, but require the addition of lead to make them melt at ^05.

I can strongly recommend "Black Gold Matte" which is available in our "Insight-Live Glaze Database".  It's well-behaved in that it doesn't run all over the place at ^6.  If you want a runny gold, you want "Saturation Gold" which is also in the glaze database. 

If you want a low-fire gold I'd suggest buying a pint of Western Pottery "Aztec Gold" rather than mixing a lead based glaze yourself. The example photo shows a nonuniform surface which is rarely the case. It is more typically a uniform bright gold color.   http://shop.clay-planet.com/pint-722-aztec-gold.aspx

As with gold lusters used at ^016, copper and cobalt are used in varying amounts to change the shade of the gold color. Reduce the percentage of manganese dioxide and you get "Gunmetal Black", also in our glaze database.

Gold Black Matte  ^6
Redart Clay 49.000 35.90%
Manganese Dioxide 35.000 25.64%
Ball Clay 40.000 29.30%
Silica 4.000 2.93%
Bentonite 2.000 1.47%
Copper Oxide Black 4.000 2.93%
Cobalt Oxide 2.500

1.83%

Hi Norm,

Good info!  However, I definitely need something without lead.  And I fire to ^6.  My teacher may or may not share her recipe,  I wanted to see if there are alternatives,  just in case.  Below is a header for a website I'm making for her with an example.

Thanks!

Norm Stuart said:

Gold glazes, to the best of my knowledge, all have very high percentages of manganese dioxide with small amounts of iron. Most of these recipes become extremely fluid, but require the addition of lead to make them melt at ^05.

I can strongly recommend "Black Gold Matte" which is available in our "Insight-Live Glaze Database".  It's well-behaved in that it doesn't run all over the place at ^6.  If you want a runny gold, you want "Saturation Gold" which is also in the glaze database. 

If you want a low-fire gold I'd suggest buying a pint of Western Pottery "Aztec Gold" rather than mixing a lead based glaze yourself. The example photo shows a nonuniform surface which is rarely the case. It is more typically a uniform bright gold color.   http://shop.clay-planet.com/pint-722-aztec-gold.aspx

As with gold lusters used at ^016, copper and cobalt are used in varying amounts to change the shade of the gold color. Reduce the percentage of manganese dioxide and you get "Gunmetal Black", also in our glaze database.

Gold Black Matte  ^6
Redart Clay 49.000 35.90%
Manganese Dioxide 35.000 25.64%
Ball Clay 40.000 29.30%
Silica 4.000 2.93%
Bentonite 2.000 1.47%
Copper Oxide Black 4.000 2.93%
Cobalt Oxide 2.500

1.83%

Attachments:

The photo you have supplied title beautiful handmade pottery is not a manganese dioxide Gold glaze. This is a photo of the Gold Black Matte.  I'd suggest you take some time to browse through the images in the glaze database to become familiar with what is possible.

Another method is to use an underglaze which provides movement to the glaze on top.  This is a bowl made with Randy's Red over Strontium Crystal Magic underglaze posted by another member here.

Some at our studio apply a wash of Potassium Carbonate (pearl ash) or Sodium Carbonate (soda ash) over their glaze to create movement, particularly over our style of studio made colored underglazes.

Your sample photo. I'd guess your teacher has applied rutile, or a very fluid iron rutile glaze on the rim.

http://storage.ning.com/topology/rest/1.0/file/get/3127169901?profile=original

Sherri Donlon said:

Hi Norm,

Good info!  However, I definitely need something without lead.  And I fire to ^6.  My teacher may or may not share her recipe,  I wanted to see if there are alternatives,  just in case.  Below is a header for a website I'm making for her with an example.

Thanks!

Norm Stuart said:

Gold glazes, to the best of my knowledge, all have very high percentages of manganese dioxide with small amounts of iron. Most of these recipes become extremely fluid, but require the addition of lead to make them melt at ^05.

I can strongly recommend "Black Gold Matte" which is available in our "Insight-Live Glaze Database".  It's well-behaved in that it doesn't run all over the place at ^6.  If you want a runny gold, you want "Saturation Gold" which is also in the glaze database. 

If you want a low-fire gold I'd suggest buying a pint of Western Pottery "Aztec Gold" rather than mixing a lead based glaze yourself. The example photo shows a nonuniform surface which is rarely the case. It is more typically a uniform bright gold color.   http://shop.clay-planet.com/pint-722-aztec-gold.aspx

As with gold lusters used at ^016, copper and cobalt are used in varying amounts to change the shade of the gold color. Reduce the percentage of manganese dioxide and you get "Gunmetal Black", also in our glaze database.

Gold Black Matte  ^6
Redart Clay 49.000 35.90%
Manganese Dioxide 35.000 25.64%
Ball Clay 40.000 29.30%
Silica 4.000 2.93%
Bentonite 2.000 1.47%
Copper Oxide Black 4.000 2.93%
Cobalt Oxide 2.500

1.83%

Can you please tell me the recipe for the soda ash wash?  How much soda ash to a cup or water or something like that?  Are there any other ingredients? I really want to try this over some of my glazes.

Thanks,

Judy Smith

Norm Stuart said:

Some at our studio apply a wash of Potassium Carbonate (pearl ash) or Sodium Carbonate (soda ash) over their glaze to create movement, particularly over our style of studio made colored underglazes.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service