June Perry's Discussions (39)

Discussions Replied To (17) Replies Latest Activity

Stars

"Jan, here's the corrected text, with a larger photo. If you click on the photo it sh…"

June Perry replied Jul 19, 2011 to CORRECTED LIST AND NEW PHOTO OF CONE 6 TESTS

5 Apr 14, 2012
Reply by Darthe Hues

Stars

"Jan, the schedule I used was to hold an hour at cone 6, drop down to 1700F, then fir…"

June Perry replied Jul 18, 2011 to Jan Wallace Cone 6 Test Results

14 Feb 1, 2012
Reply by Benjamin Coffman

Stars

"I don't think you can look at someone's tests, especially when they're layered, to k…"

June Perry replied Jul 17, 2011 to Jan Wallace Cone 6 Test Results

14 Feb 1, 2012
Reply by Benjamin Coffman

Stars

"It is weird. I can get them on my HP laptop, but not on my Dell Xps, even though bot…"

June Perry replied Jul 16, 2011 to Jan Wallace Cone 6 Test Results

14 Feb 1, 2012
Reply by Benjamin Coffman

Stars

"Jan, I scrolled down but no pictures are showing up. Are the photo of the tests in a…"

June Perry replied Jul 16, 2011 to Jan Wallace Cone 6 Test Results

14 Feb 1, 2012
Reply by Benjamin Coffman

"Alfred University will test. A few years ago they were charging $15 to test for each…"

June Perry replied Jul 10, 2011 to Testing Glazes for Durability, Fit, and Toxicity on Functional Ware

11 Mar 15, 2015
Reply by Norm Stuart

"It depends on your base glaze Jeff. 1-3% red iron in the right base, with a little t…"

June Perry replied Jul 5, 2011 to Yellow Matte

28 Jul 5, 2011
Reply by June Perry

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service