I'm trying a new project and I was wondering if anyone had any experience or advice. I want to make some seamless porcelain rings like these by Monika Skrzypkow. I don't want to copy her work I just want to figure out how to make the blanks and then I can add my own touches. I found a mold that is used with metal clay but am unsure if it will work for porcelain, the manufacture wasn't sure either.

If anyone can shed some light on this I would really appreciate it.

Thanks

Views: 492

▶ Reply to This

Replies to This Discussion

Depending on size -- finger rings? napkin rings? bracelets? larger? Throw tall cylinders. Profile into sections with a custom rib (old gift card , etc. cut to shape), but don't cut completely through until they are close to leather hard. You could do some exterior decoration before cutting them apart. 

Extrude a tube and cut it up and smooth the edges.

Find a cylinder the size of the inside hole you want before shrinkage. Wrap carefully in paper so there are no wrinkles. Slab clay to proper thickness and cut strips at the proper width. Wrap, cut edges at a diagonal to fit together, score and attach. Remove from mold before they get too dry or the shrinkage will break them, but the paper will slide right off without causing distortion of the clay. Trim corners and shape at leather hard. Smooth at dry.

If you have a wheel, high level production would be better by George's suggestion.

Thanks for the replies, as I don't have a proper extruder I think I will try and throw a slim cylinder and go from there.
Thanks again.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service