I wanted to ask if anyone has a good way to fire glazed ornaments?  I hung mine from high temp wire on a bead bar.  The bead bar warped and all the ornaments sagged and fused together.  The bead bar was suppose to be strong enough for a cone 6 fire which is used.  Any help will be greatly appreciated.

Views: 248

▶ Reply to This

Replies to This Discussion

I bought some heavy duty rods, cut them in half & stuck them in a soft brick. I did this to several bricks.  This next year, I am going to buy some more rods & drill holes & put the rods in a hard shelf.  

The rods are from Kemper & are CBBH bars.  They are 11" long & $6.45/each for 6 or more.  I might try the ceramic rods for the high fire bead rack.  I think they are only $1.40/each.  When you cut the metal ones in half, they are only 5 1/2" long. That works for most ornaments if you don't push them too far down in the soft brick.  The ceramic ones are 6" long & they might work better putting them in a hard shelf.  jhp

Thank you Jeff for your response, I will give it a try with the ceramic rods you suggested.  Love the beautiful work in your picture:)...Tracy

Thanks Tracy!  Bear in mind that I have not taken these to ^10, but only to ^5.  They say that they will go to ^10, but I haven't had a need to do that yet.  The ones I made last month are only going to ^3.  I haven't finished any yet, but will post pictures when they are done(assuming that they aren't hideous!).  I haven't gotten them all poured yet, nor bisqued(soft), cleaned, underglazed, re-bisqued, & then glaze fired.  It's a long process, & I got a late start.  The good thing is that I now have my own molds & can make ornaments on my own time & process.  jhp

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service