Hi All,

As an Aussie I find it frustrating that so many of your lovely glaze recipes require Gertsley Borate which, I understand, is in very short supply. I would love to see more recipes reformulated to include more readily available ingredients, particularly for us poor souls 'down under'.

Greetings to all from Western Australia!!

Clive

Views: 742

▶ Reply to This

Replies to This Discussion

Have you seen Tony Hansen's pages on gerstley borate? http://digitalfire.com/gerstleyborate/substitutes.html

As we now have an assured supply of fairly consistent composition gerstley borate, there is less pressure on US potters to find alternatives. If you are in the US and use glaze calculation software, you might want to update your composition from the 1997 or 99 formulations to the currently published formulation found at http://www.lagunaclay.com/support/pdf/Chemical_Composition_of_Gerst...

Importing Laguna's Gerstley Borate from Laguna Clay, the company which now owns the Gerstley Borate name and produces this (almost certainly) blended product, is more expensive than buying it in Los Angeles for $1.94 a pound or $0.63 a pound for a fifty pound bag.

http://wc.strategyonline.com/BA390.500/Gerstley-Borate-_dash_-Natur...

Where do you buy ceramic supplies on the west coast? Someplace in Perth?

In the past some have suggested Ferro Frit of Australia's 4112 frit as a substitute.

http://digitalfire.com/4sight/material/ferro_frit_4112_2389.html

The one real advantage of Gerstely Borate over a frit is that its clay-like properties suspend the resulting glaze.

Looking at the finished products, there's obviously someplace to get stuff:

http://www.ceramicartswa.asn.au/gallery

walker ceramics in melbourne Phone 03 87616322

$10.oo per kg in small quantities

$140 for a bag of 22Kg

Transport costs might be a problem

cheers Ivan

Thanks for that info Ivan - I will check out Walkers when I am next in Melbourne.

Cheers!

Thanks George!

At the moment I am happy with my glazes that don't need GB, but it is tantalizing to see such nice glazes from you guys in the States and not being able to try them myself. I will check out Tony Hansen's page - always educational stuff to be found on his site!

Cheers!

Hi,
I'm up in Cairns, FNQ. We order online having no supplier up here. Haven't had any problems with Gerstley Borate though.

You could try the Clayshed on the Sunshine Coast, they are really helpful.

Cheers,

Jenny

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service