I am hoping that you all may be able to help me through my next phase.  I began at a pottery studio 8 months ago.  To say that I've fallen in love with pottery is an understatement.  So I took the next step. . . I have an 8 x 12 shed with a wheel and a wedging table and cabinet.  I'm throwing like a madwoman!  I've even taken my wheel out on our deck overlooking the Maine woods - nirvana!

 

So I have that down and it's time to fire up the used kiln I bought.  It is a GARE electric with a kiln sitter that can go to cone 10.  I

I am used to working with cone 10 clay and I love the 550 porcelain.  I've worked with 910 (too groggy) 700 (better) BMix, and two white clays (can't remember).  I found that b-mix at the studio seemed to pull out so much gray in the glazes so celadon was AWFUL. 

Working with glazes (cone 5/6) is all new.  I can't afford the dry (25lbs???) and do not want to invest in something until I am sure 

So I am reaching out to kindhearted potters for help. Advice about the first firing, the best glazes (I tend to like pastels), the best clay (I prefer white and porcelain).  My pottery studio also has a supply that is well stocked. 

I look forward to learning and maybe some day being able to know enough to pay it forward.

Views: 194

▶ Reply to This

Replies to This Discussion

Tess,

You'll get a lot more help on this active forum:

http://ceramicartsdaily.org/community/forum/19-ceramic-arts-daily-f...

Good luck.

John255

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service