The potter in the video has probably mixed the clay he is using with a Mason Stain colorant or metal oxide or carbonate colorant. Since the clay bowl is still very wet, this slip will adhere fairly well.

But this colored slip layer can sometimes become detached or cracked as the bowl dries, or when it is bisque fired. This is why slip-trailing recipes always add a flux to help melt the slip to the bowl in the kiln. There's not much difference between a slip-trailing recipe and an englobe recipe.

I wasn't surprised when I read a page on the Frog Pond Pottery site (John Hesselberth co-author of "Mastering Cone 6 Glazes") which tested commercial under-glazes and found almost all of them blister-off the ceramic when fired. This is why englobes and slip-trailing recipes often contain flux material, something that melts in the kiln to glue the color to the clay.

Underglaze is a colorant (Mason Stain, metal oxide, or metal carbonate) mixed with clay (kaolin and silica) and water. Clay doesn't melt nor do colorants. Kaolin mixed with colorant will also has a different drying and thermal expansion characteristic than each clay that you use.

After reading Hesselberth's tests, we began making our own "underglazes" by mixing two parts of Laguna Gerstley Borate with one part Mason Stain colorant and six parts water.

This is not a glaze, but the boron in the gerstley borate melts just enough to securely adhere the color to the greenware or bisque when it's bisque fired. Even if it is slightly detached when dry, it will lay down and adhere in the kiln. People can then apply low-fire or high fire glazes over these colors, often a clear, and the colors don't run or mix into the glaze.

We also mix these color concentrates with a low-fire or high-fire clear glaze to make a colored glaze.

The flux materials added to the trailing-slip in this Ceramics Daily article are:

Talc
Calcium Borate (or Frit 3110)
Nepheline Syenite
Borax

http://ceramicartsdaily.org/ceramic-supplies/ceramic-raw-materials/...

The "underglaze" ingredients are:

Kaolin
Calcined Kaolin
Silica
Zircopax

If you use only the underglaze ingredients without adding the flux ingredients, you will probably encounter problems with the slip blistering-off the bowl.

Just start using your englobe and you'll quickly see if you need to make any changes.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service