Does anyone use a "Loading Ring" on their top-loading kiln to protect the top firebricks from damage?

Are loading rings commercially available or do we need to buy some plywood and have it cut with a jigsaw?

Our kiln is frequently loaded by inexperienced people who find it very easy to break the top ring of firebrick, either hitting it with ware or leaning on it with their hand or arm.

They're easy enough to repair or replace with 1.51 parts of Wollastonite mixed with 1 part of Phosphoric Acid 80% concentration, but it would be nicer to prevent to problem in the first place - as the repairs inevitably spall-off the brick within a year.

Wollastonite & Phosphoric Acid

Views: 288

Reply to This

Replies to This Discussion

Interesting - The studio I teach in needs them .

"Loading Ring" (photo) to protect the firebrick in our top-loading kiln.

In place to load the kiln. We bought a plywood round and had the inside cut with a jigsaw.

Precariously laid on the kiln edge to display the wood blocks which hold it in place.

Nice - thanks for the pictures- really good idea

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service