I am debating putting a downdraft vent on my Skutt 1027.  I don't need it for health reasons, my kiln is under an outdoor shed roof.  I am hoping it will even out the cones from top to bottom, and improve colors.  Bottom is almost a cone cooler sometimes.  I always have at least 4" posts on the bottom shelf and 2" posts UNDER the bottom on the kiln floor.  I keep the bottom peep in and remove the 2nd and 5th peps.

Have any of you added a vent after firing your kiln without?  What did it change , or not have any effect.

Views: 264

▶ Reply to This

Replies to This Discussion

I added a vent system many years ago and found that my colors were better,  more vibrant.  I fire with an electronic controller and I put a separate pyrometer in the top also.  The top pyrometer is always 100 degrees hotter than the electonic display.  The biggest improvement for me is the environment,  my kiln is in the garage and I don't get any fumes with the vent.  My smaller kiln is unvented and you can really smell the difference,  especially in bisque fire.

If your kiln is in the open then you may want to think about all that shelf mass (weight) in the bottom to heat.  Its a surprise you only one cone cooler.

If you know your glazes, and with a good coat of kiln wash, you can use the bottom and eliminate the protection shelf.  If you still feel cautious about using the bottom make small slabs with fire clay to set pieces on.  Also the slower the firing the better distribution of heat work.  Soaking at the top may do as much, or more for your glazes than ventilation while also evening out the heat distribution. Worth a try  Good luck with that.

John255

 

I'm curious what your witness cones would indicate if you fired your kiln with just one peephole open.

Your 7 cu/ft kiln is twice as large as ours but puts out only 33% more wattage. We had an older kiln with this lower heat to volume ratio which fired unevenly, according to our witness cones.

Someone mistakenly fired our new kiln with both peepholes open (we have only two) and the bottom of our kiln was well more than one cone cooler and the top shelf was too hot. Our one thermocouple is in the middle of the kiln.

For better or worse we place three 3/8" thick pancakes under the bottom shelf. This places the side of the bottom shelf directly in front of the bottom row of elements (each 4.5" tall layer of firebrick contains two rows of elements). This arrangement provided us with even witness cones placed on the bottom, middle and top shelves. Far better than laying the bottom shelf directly on the firebrick floor.

Being outdoors we don't have an exhaust fan on the kiln. This means I can deliberately lightly pink a tin white majolica by placing a chrome glazed pot on the same shelf, but with the chrome glazed piece placed higher in elevation than the white majolica to be pinked. So obviously we need to load the kiln with this cross-contamination in mind when it's not desirable.

The pink color of cross-contamination on tin white majolica, from a chrome glazed pot placed on a half-shelf above the plate.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service