Is firing at a higher temperature for bisque than for glaze really that unheard of?

It's the way I was taught and have been firing. I've been working out of my home studio for the past three years, and the ceramists and potters in this area are often downright rude about how I am "doing it wrong."

I like the work I make and people buy and use it. In that sense, I'm not doing it wrong.

It seems like there should be at least some school of thought that coincides with what I was taught. Where is it hiding?

NOTE: Replies are posted from oldest to newest, so the most recent posts will be at the bottom of the last page.

Views: 4164

Reply to This

Replies to This Discussion

Test tiles are always a great idea. The most common change I've seen in cone 6 glazes refired to cone 06 is a reduction in their glossiness.

We all know some ceramicists are quite snobbish about the "wonderful" look of glazes fired to cone 10 where many of the coloring oxides partially evaporate, but that's just one look.

I'm fascinated by the incredible variation in how industry makes china or dinner ware. This first method at Coors uses once-fire where the glaze is applied to the greenware, then fired once at cone 2.

http://www.youtube.com/watch?v=hfv2TPxf-gg

This second method at Lenox fires the bisque to cone 9, polishes the bisque, then heats the fired bisque, applies glaze and refires to cone 6.

http://science.howstuffworks.com/innovation/51-how-fine-china-is-ma...

A third method bisques slip-cast porcelain at cone 06, then applies enamel and refires the ware to cone 14.

http://www.youtube.com/watch?v=isANl_4YPUQ

Another method, I can't find the video for at the moment, vitrifies the unglazed china at cone 12 on slump-mold plate setters, also called chums, dusted with alumina. After polishing off excess alumina, the dry glaze is sprayed onto the electrically-charged plates and fired to cone 9. Decorations are then added and refired to cone 016.

This ceramic PhD discusses dealing with the problems of shrinkage, slump, and drag at very high cone firings.

http://ezinearticles.com/?Ceramic-and-Pottery-Defects-5:-Defects-Ge...

There's so many different ways to get something done. In southern California I've found the most arrogant and snobbish ceramic artists often don't even know how to make their own glazes. When people don't know much about a subject they sometimes develop rigid and simplistic opinions about "the right way" to do something.

We used to have a book at our studio which showed the work of several ceramic artists whose work was the result of eight to fourteen firings at different kiln temperatures. They had incredible depth and complexity.

I had people tell me when I started working in clay that it was a huge mistake to refire pieces but I tried it with pieces I wasn't satisfied with and now I do it regularly.  If I can't make it right, it will go into the shard pile anyway. 

There are those glazes that do not take kindly to re-firing.  I have not been able to come up with a hard & fast rule about which ones do & don't.  I did a test with 32 different iron reds & there were several of those that pitted & some were dull & some that went clear as a result of the re-fire.  There were those that came out way better than before.  I would have to know what was in all 32 glazes in order to make sense out of the results, & since quite a few of them were commercial glazes, that would not be possible. If you don't like how a pot came out, you certainly don't have anything to lose by re-firing it.  Now, if you kind of like it, you may be disappointed by how it comes out on the re-fire.  So choose wisely!  I have had a few that I wish I had left alone after the first fire.  Also you have to remember that the more times you stress the clay, the greater chance you have of breaking it.  If there are imperfections, they are more likely to crack &/or break the more times that you fire them.  jhp

This artist uses multiple firings to good effect.

http://www.hubertceramics.com/vases

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service