Im considering switching my clay to little loafers. I need to find a good clear glaze to go over slip decorations.

I'm going to test what I have, of course, but if anyone uses a clear glaze with good success on this clay body I'd really appreciate suggestions.

Thanks!

Views: 1128

▶ Reply to This

Replies to This Discussion

I mix my own clay so I do not know if this will fit Little  Loafers.  You could test it to see. Plan on putting these into insight. I didn't check to see if they are in the data base or not.  The M--# is my own system of keeping track of my glazes. M--104 Clear; cone 6, Dolomite 17,Custar Feld 34.10 Ferro frit 3134 14.9, EPK 17, silica 17.   also    M--105 Clear; cone 6, Ferro Frit 3195 31, Dolomite 14, EPK 19, Flint 36. These fit my clay real well. Happy firing

Thanks!

Hey Leigh, If you try these two clear glazes and they do fit, please let me know and I will add it to the notes when I add these to Insight live. If you would please  I am going to add my clay boby recipe in the notes when I put a glaze in the data base. Thank you. Happy Firing.

My test is done, and I'm happy to report that almost everything worked on little loafers. What I did was made a bunch of cups about 4" tall, 3" diameter. I bisqued them to 04 and then poured my test glazes on the inside and brushed 3 coats on the outside.

Here are the glazes I tested in this round:

G1214W- clear low expansion glaze from Tony Hansen's digital fire site, I used g-200 feldspar instead of Kona F4 (COE 66.13)
Glossy Clear Liner from M^6 Glazes (COE 67.92)
TUC-C, variation of Tony's Ultra Clear (COE 67.21)
Standard 1199, commercial glaze that standard sent me to test

The recipe for TUC-C is EPK 21.8, G-200 17.4, Frit 3134 26.1, Silica 21.8, Wollastonite 8.7, Talc 4.2.

The kiln fired to about cone 7. I wanted to go to cone 6, but I'm still learning my new kiln.

I tested the cups for crazing by alternating plunging them in boiling water and ice water 3 times. None of the glazes crazed on Little Loafers.

The only glaze that gave any problems was the commercial 1199 glaze. It didn't craze, but it did pinhole on the inside of the cup, which I had also previously seen on top of another clay body. It could be due to the kiln firing closer to cone 7 than cone 6.

I also tested whether my slips (made from Standard 182 without grog) would fit on top of Little Loafers. Small test cups were coated with about 5 layers of slip and then carved off a little to try to simulate my normal technique. A couple of the different glazes above were tested on the cups, and they all look fine. The slip didn't crack or peel off, and the glazes looked great.

Kabe- if I get around to testing your glazes I will let you know if they fit. I don't have dolomite, so I'd have to get some first.

*note- the COEs were all determined in Glazemaster. I think some programs give different results for the COE calculations.
Oh, I also included some test bars of standard 182, Little Loafers, and Standard 240 to do absorbance tests on them. I'm interested to see the absorbance of LL compared to Standard 182, and see if that could be the reason I couldn't get rid of the crazing on the 182.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service