I just started making my own glazes again this year. Before that, it had been about ten years. At that time, Gerstley Borate and Kona F4 Feldspar were still being mined.

Many recipes still call for these. My understanding is that people have many different opinions on substitutions. My local pottery uses a straight one-for-one substitutions with Gillespie Borate and Minspar.

I'm curious what your experiences have been.

Views: 2413

▶ Reply to This

Replies to This Discussion

My suggestion would be to install the Glaze Master software (they provide a 60 day free trial) perform an analysis of your old formula and then substitute the GB with another ingredient and you will see exactly what it does to the glaze from a chemical standpoint. The software allows one to review the makeup of the various minerals individually which would let you choose a substitute that is the closest possible substitute. That software is very easy to learn. What I really appreciate about it is that it has minimum an maximum values that let you know if you will create a glaze that will be strong or weak re silica (strength) and alumina (enough to melt the silicates without running. That software allowed me to better understand glaze chemistry. Robbin Hopper's glaze book, can't remember the name, is the best for learning along with the software. Good luck!

WOW! What a great resource!

Hi Shine. You may have solved your Gerstley Borate questions by now but I came across some stuff called Laguna Borate. Which I think was made to fill the gap created by the absence of Gerstley. When I make the one for one exchange on my Digital fire software the chemistry is very similar. I have not fired a tile yet to compare visual results but I will soon. Happy firing

thank you--- sorry for the extremely slow reply

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service