Joanna said on July 24, 2012:

"I am fairly new to pottery and would really love to know how one goes about glazing a piece so that there is no white foot visible at the bottom of the pots.  I keep noticing and admiring various members work where the glaze reaches all the way down to the bottom of the piece, even on glazes that are known to be runny.  I really dislike the white band (no matter how narrow I get it) at the base of my pieces.  I have tried taping the foot and waxing a very small foot, dipping into wax or just freehand on the wheel.   And yes there is always that dreaded white band.  Any words of wisdom or advice would be apprecaited!"

The first reply came in from Jeff Poulter a bit later on 7/24/2012:

"I have a few ideas. I use the ultimate edger to put a rounded foot on each piece I throw. I spray my glazes so you can get just the right amount clear down to the foot and I stilt everything in the glaze firing. I use Roselli stilts and just clip the little metal prongs off as they will deform at cone 5/6 and your pot could tip over(learned that the hard way!) Hope these ideas help."

Joanna replied back again on 7/24

"Jeff - Thank you for your reply!  That was what I thought I should be doing. I do use the ultimate edger myself, love it!  I am planning on ding a more spraying now that I have everything working at home.  I will look into the slit idea as my mind was wondering about that too!  Funny you should reply it was your red flared bowl that made me finally ask!  Love it! Looking forward to the pictures after your bisque fire. thank you! jo

I have another method, and we will likely get more, so I have moved this conversation to a discussion page of its own.

Views: 749

Reply to This

Replies to This Discussion

Steven Hill taught me his foot technique, and I use it for about 90% of my pots. It involves leaving an expanded "glaze catcher" ring at the foot, and then using a trimming tool to cut a very shallow angled undercut beneath the glaze catcher so the pot appears to float off the surface just a bit. Using the technique also gives you the advantage of not having to trim a foot ring. The top of the glaze catcher extends out horizontally from the wall of the vessel and is rounded over to make a chip resistant rim. It is remarkable how much glaze will collect in the glaze catcher, before spilling over the edge. It will then have to gather more quantity before it will run totally off the pot.

With my smaller pots, the angled undercut extends for about a half inch from the glaze catcher to the actual bottom of the foot. I can then use wax resist half way out the undercut, or all the way to the bottom surface of the glaze catcher to determine where the glaze stops.

I have heard (and have not tried) using a layer of sand on the kiln shelf will allow you to glaze all over without the piece sticking to the shelf. It doesn't sound so different from what Brian suggests with the shells.

In terms of cleaning a piece up after having glazed it, buttons have given me a lot of practice cleaning off the bottom without losing much glaze on the sides. After the glazed piece is dry-- completely dry-- I spray water onto a bat or ware board. It should be thick enough that the entire board is covered but not so thick that it doesn't break its own surface tension. I allow the piece to rest in that water for a few minutes, and the glaze washes off easily where it was wet.

I can only speak for how well this technique works for vitrified ware. I would be curious to hear how it acts with porous bisque.

George - thanks for your reply.  I will give this a try!

 

Brian - thank you too! I like the hidden foot idea and think I'll go with that.  I was intrigued with the sea shell concept though.  How did you ever come up with it?

Shine - Hello and thanks for the imput.  I have heard of the sand idea.  A friend actually mixes the sand into his wax and then when the glaze run is over the piece is sitting in sand. 

 

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service