Comment by Tracy Minarik - Steven uses Standard 257 porcelain.  I use it now also, but have trouble attaching handles.  Everything seems to crack.  Been doing handles on cups for 15 years. Don't get it??  I'm going to try some "Magic Water" by Tony Clennell next.. We'll see........

Comment by Wanda Manning - Just attended a two day seminar with Steven Hill and he does not use anything but magic water to attach his handles. He made the comment when he used slip he could get cracks also
Comment by George Lewter -  I'm not using porcelain (b-mix 5 instead). I stopped slipping and scoring about 6 months ago. I use 2 parts water to 1 part white vinegar painted on the surfaces to be joined and I just wiggle and lightly mush the parts together. I have a concern about the sodium silicate in magic water causing a glaze to not absorb at the same rate (thickness) as on pure clay.
Comment by Joe Shaw - I use slip to attach handles and the like. I "wiggle" them in place. What I've found it that it's necessary for me (I work with porcelain) that my pieces dry slowly. My wife and I went to a restaurant supply store and we found an old two door stainless steel cooler/refrigerator for dirt cheap. Plastic interior, shelves and (most importantly) doors with gaskets in good shape. I really need to slow down/control drying especially when doing slip decoration. This applies to handles and such also. When one recycles clay as I do, vinegar can be an issue, it helps to create and ungodly stench in the slip barrel.
Comment by George Lewter - The tiny bit of vinegar water I use for attaching handles shouldn't be going into the slip barrel unless I break the piece.
Comment by Joe Shaw - I use Laguna's Frost and Clay Planet's Icelia porcelain. Both fire to translucent. I've suffered with cracking with both clays until I got a grip on the damp-box and controlling the drying.

Views: 418

▶ Reply to This

Replies to This Discussion

Hello, I am new to this site, kinda wandering around peeking at discussions.  My husband Paul is a production potter, and I have added a video of his handle method to my page here.  This video uses stoneware clay, but he uses the exact same process with porcelain.  When he encountered cracking at one shop where he used porcelain, along with slow drying,  they started to paint the joint area with a latex wax resist after attaching which burnt off in the bisque.  

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service