Need help with Pure Brilliance Glaze on Terracotta, PINHOLING problems

I have had good experiences with this glaze in the past, and now seem to be encountering difficulty with pinholing, most especially on large plates and platters - almost a given.  Other forms seem to be fine.

The viscosity I use is approximately 21. Currently I am doing a mix of brushing application and pouring liners and flatware to achieve a uniform surface.  This has been a standard method for me that has worked in the past.  I am firing to a hot 04 bisque and glazing at 05.  I have never found the need to soak, however I do close the top spyhole immediately when kiln shuts off.  I do a slow firing approximately 10 hours and give ample time for cooling. I have an older model Skutt kiln model 231 that fires consistently even in temperature – manual controls.

In the past I have had success even with the platters, but now am troubleshooting.  Would love some help as my dinnerware orders are stalled in production, and pottery is my living with summer fair season already here. 

Thank you for any advice from a desperate Montana potter. 

Views: 267

▶ Reply to This

Replies to This Discussion

Thanks, Brian.  remembering my early days of stoneware/gas kiln firing, i would see that adding a flux to the mix would help it move slightly.   OK. I use a commercial glaze that arrives in gallon format.  How would i go about figuring 1 percent of the total, adding a dry ingredient into the liquid?   The total gallon is about 128 oz.  As an artist, this is beyond me, but as a cook, i'd say throw in a pinch!   However, i do want to be a bit more accurate.  Ideas?    I actually happen to have gerstley on hand.   I just finished up a firing to a high 04 and will use the same method when firing my 05 glaze so it also goes a bit higher.  Just adjusted the claw on the kiln sitter to catch a bit more of the bar and thus go a bit higher.    A question on soaking.  If i immediately turn the kiln back on once it shuts down, to say MED. for 30 mins or so, I assume the top spy hole should stay open until i shut it off?  Or should i close it down during the medium soak ?    thanks for your thoughts.  I do not have an additional venting system.       Joanna  

thanks so much!  That was the general picture that was in my head re the mixing in of the powder... thanks for making it lucid.  The reason i asked about the venting system is that i visited a studio yesterday to drop off a platter to see how their usage of the same glaze might turn out... they use the same glaze effectively on commercially bisqued molds.  Their newer computerized kiln has an "Envirovent system" pulling fumes from the bottom of the kiln and thus they always keep ALL the spy holes closed through the whole glaze firing.  I have also come across info in my research that talks about effective burnout of organic materials, especially in terracotta, that is aided by this venting downdraft system.  Also aiding in elimination of pinholes.   One suggestion was to keep all spyholes open all through the firing up until red heat begins, to provide adequate oxygen for complete burnout.   What are your thoughts on this?  haven't tested this method.     I really appreciate having someone to bounce  questions off of :)  !    

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service