I'd like some help learning to fire an Evenheat 4320 with kiln sitter...

I bought a used Evenheat 4320 kiln with kiln sitter.  It does not have knobs to adjust heat settings.  I has 4 switches that you turn on one at a time.  I'd like to fire to cone 6 or cone 5 with a soak.  Never having fired my own pottery before, I don't know how to go about doing this, much less with this type of kiln.  I fully intend to learn how to fire successfully.  So, anybody willing to give me some pointers?  I can use all the help I can get!  

Views: 5427

▶ Reply to This

Replies to This Discussion

The Users Manual I found for your kiln is attached. There was not a lot of info about the switched variety except:

"Kiln models equipped with ON-OFF toggle switches generally have two or more switches. Standard operation is to throw the bottom switch to the ON position while leaving all remaining switches OFF. 

Allow the kiln to fire for one hour. Once the hour is complete, throw the next switch up from the bottom
to the ON position, again leaving all remaining switches OFF. Allow the kiln to continue to fire for
another hour. Repeat this process for all remaining switches and allow the firing to complete.
It should be noted that you may fire faster or slower by adjusting the amount of time you wait
before throwing the switches to the ON position."

You will have no idea what your kiln is doing unless you get a pyrometer and thermocouple to measure the heat inside the kiln. 

Test your kiln by turning all switches ON wait 5 minutes and look in to make sure all elements are glowing. Shut off the switches one by one (again waiting a few minutes) to see which switches control which elements. Make notes if they are not 1 switch for 1 element. 

Read the manual. First learn to do a controlled fire (heat up at a desired rate, learning how your kiln responds to the switches at low temperatures and especially at high temperatures).  Then you will need to be switching on and off one or more of the switches on a timed basis to hover around a desired temperature to do a soak. You will not be able do a soak without a pyrometer. 

Attachments:

Thank you so much George.  I intend to do an empty fire of the kiln to ^6 before I do any real firing.  Since I bought it used I want to make sure it goes up to temperature.  After that I guess I'll just have to trust the kiln sitter until I can get a pyrometer and thermocouple.  I'm dying to try out some new glazes that I bought!

Hi Renee,

I have a Duncan Teacher Plus with a kiln sitter. You do not necessarily have to 'trust the kiln sitter." You can use witness cones.

A side note that might help you in the future: It took me a little problem solving to figure out how to soak my pieces at the top temperature without having the kiln shut off on me. I put a cone seven bar in the kiln sitter and watch my pyrometer VERY CAREFULLY. At that point I can manually turn the kiln down a bit so it doesn't go above cone six or shut off and hold it there with a little tweaking. Of course, this is a pain in the behind, but for me it is worth it. I like to cool everything down slowly because I find I get much nicer depth to my glazes, rather than having the kiln just shut off and cool down quickly. You should be able to turn your kiln down gradually too if you can prevent it from shutting off.

My husband said someday he will convert it to digital for me, but he thinks I should have to do it the hard way first! LOL! I suppose he is right. It is a great learning experience. I hope you enjoy your kiln and all the learning that goes with it too! Read the manual a couple times, and then stick it up on the shelf and forget it! You will gain much more from your own trial and error and firing logs. : )

Jen

Thanks Jen.

I have an old evenheat with 5  toggle switches and a kilnsitter. Does yours have a plate that states the volts, amps and max temp?  I would not be sure that yours would go to cone six..depending on the elements.  Mine has been great for quick bisque turnaround for many yrs.

George...thanks for the pdf manual, I will check it out... Oh well, it does not apply to the old toggle switch models.

Mine went to cone 6 empty so ]'m hoping it will do it full. Mine has for toggle switches I think. I haven't had the chance to do a glaze fire yet. I'm visiting my mother for the summer. I sure do miss my clay though.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service