As a starting point, here is a list of online sources of cone 6 glaze recipes. It has been moved over from its former page, to help organize glaze topics under discussion categories.

 

Group 1 - Having both photographs and commentary on the glazes.

  •  John Post generously shares his glaze research, and coats his simple forms with spectacular glazes. His website is arguably the best cone 6 glaze resource currently online. He has extensive information on a technique of glaze testing.
  • Alisa Clausen has the most extensive photo-documented cone 6 dedicated glaze recipe Website that I have found. Most of the recipes are for cone 6 glazes. The right column of her page links to groups of glaze tests. Her source of recipes is largely the Sankey Glaze Database which is available right here on our network.
  • John Anthony's Red Hill Pottery has some great shots and notes on his tests of many published recipes.
  • June Perry does extensive glaze testing and shares her results generously on her Website.
  • James Jacobs has a set of ^6 recipes with pictures on his Website. Caution -- all of the photos of finished examples were fired in reduction. He says only the cobalt blues and heavy iron formulas would be useful in oxidation.

Group 2 Recipes not as well documented as Group 1

  • The clayart discussions at potters.org are a prodigous source of ^6 glaze recipes, but you won't find pictures here. Some of the discussions give links to Websites with pictures, but generally you will only find recipes and written descriptions of glaze characteristics. The SDSU ceramicsweb glazebase seems to be offline. The creator of GlazeChem glaze calculation software downloaded the entire glazebase in 2001, and has it available for downloading in GlazeChem format. I've extracted the cone 6 recipes and commentary and converted it to a Word document. Here is a link for you to download the 275 page document - CeramicsWebClayartCone6Glazes.doc
  • Lakeside Pottery has an extensive list of their glaze recipes, but they refer you to their gallery to see the glazes in use without a one-to-one match up of recipe to picture. These appear to be worth exploring as they produce some very nice pieces. Update - Morty Bachar of Lakeside Pottery is now one of our members since fall of 2009.
  • Val Cushing had an article in the June 1977 issue of Studio Potter that listed a number of his recipes for glazes and engobes (or slips). Note that a number of the glazes utilize Barium Carbonate which in the intervening years has fallen from grace for it toxicity. It would be prudent not to use these glazes on the interior or mouth contact surfaces of table ware or cookware.

Group 3 Recipes lacking significant documentation.

  • I have a collection of them in a Word document totalling 61 pages. I am posting the document here for you to download and test as you like. If you do test any of them, please report your results in detail here. Good Luck. - collectedglazes.doc
  • John Wright has a list of ^6 glazes on his Web page

Let's see if our members have any interest in sharing glaze recipes. If you want to post a recipe, please follow the following guidelines.
  • Use the conventional 100 unit batch formula and the full descriptive names of all ingredients.
  • Include the source of the recipe
  • Include application methods, best thickness of application, and cautions about defects you've encountered
  • Include any special firing techniques
  • Post a picture of the fired glaze
  • If known, include the coefficient of expansion, and the clay body you've used with the glaze.

Please do not post recipes from copyrighted sources.

Views: 4701

Reply to This

Replies to This Discussion

Here is my first attempt at posting a glaze recipe. This is a mid-range celadon. I am still searching for a great celadon (blue or green) that comes close to the old cone 10 reduction celadons I used to use. If anyone has any ideas please let me know (garminpottery@gmail.com). This is a great glaze, but it is a bit too dark blue. I tried to calm it down a bit by mixing it with a clear but the result are not good.

Cone 6 Blue Celadon
Custer Feldspar 20
Gersteley Borate 20
Nepheline syenite 20
Flint 15
Wollastonite 10
Dolomite 2
EPK 5
Red Iron Oxide 2
Titanium Dioxide 1
Cobal Carbonate 0.9
Copper Carbonate 2.5

You can buy this glaze pre-mixed here : http://www.glazemixer.com/singlerecipe.aspx?RecipeID=2372
Attachments:

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service