I see no-one has started a thread in this section yet, so I'll make my very first post as a novice.  I'm most interested in sgraffito technique.  I bought some Amaco velvet underglazes, and my plan is to paint that on, do sgraffito, then bisque fire, then add a clear glaze.  I just painted some sample tiles with the underglaze while they were still leather hard, and so far so good.  Is there any reason to have to wait until the tile is bone dry before painting on the underglaze? Like if it will crack and fall off?  Obviously, the sgraffito is much easier on leather hard vs bone dry tiles, particularly for larger areas of scraping off.  

Views: 1623

▶ Reply to This

Replies to This Discussion

I sometimes work with bone dry ware and slips using scraffito when I want a crisp, tight line on the work.  I have been putting bluegrass musical instruments onto work and find that I can "draw" the strings in better on bone dry ware.

Rebekah, my experience is that underglazes go on much better "before" bone dry stage.  The bone dry item sucks the moisture from the underglaze too quickly and you end up lifting too much clay onto the brush as you work.  I use underglazes through silkscreens and don't have any luck using them on bone dry ware.  Really underglazes seem to work better for me on "set up" clay and leatherhard.  You can clean up lines and scrafitto onto the item at bone dry stage rather nicely then.  

Thanks very much.  I'll paint on the underglaze after the clay is set up, and then wait for all to get drier before I do my sgraffito.

I find it's better to do it good leather hard. Too wet and it co-mingles with the damp clay and too dry is does not create a nice bond and flakes a bit as it dries.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service