Hi everyone, I am happy to say that I just moved to Nova Scotia but am sad that I now have to look for a new porcelain as my fav, NZ6 from Clayart is unavailable here. If anyone has any recommendations or has used NZ6 and could recommend a comparable porcelain It would be much appreciated .

Views: 298

▶ Reply to This

Replies to This Discussion

Hi Brenda:

I cannot give you a specific recommendation, being unfamiliar with products in NS. I can give you some information to narrow down your search.

highly translucent porcelain bodies are formulated from New Zealand kaolin of Grolleg kaolin. For optimum clarity, V-gum T is used as the plasticizer. The supplier in your new hometown area should be able to verify these ingredients in their porcelain stock.

The other option is to review the product specifications. The COE of translucent bodies are typically higher than standard porcelain because higher levels of flux are required to produce the higher glass content. Regular porcelain averages between 5.50 to 5.75 COE, while translucent bodies run over 6.00 up to nearly 7.00.

Because high quality plasticizers are used: shrinkage values are higher. Standard porcelains run between 10.5 to 12.5%, while translucent bodies run 13 to 13.75% shrinkage.

Finally, absorption values reflect the high glass content of translucent bodies. Standard porcelain runs between 1-2% absorption! while translucent bodies are nearly zero.

happy shopping and welcome..Tom

Hi,

Where in NS are you?
Spiral Studio in Hall's Harbour owned by Terry-Lee; I'm sure she can help.
There's a lovely studio in Mahone Bay: Birdsall-Worthington
Also check in with the Nova Scotia Potters Guild.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service