Wondering which  glazes "break" best over graphics etc.

The mug displayed is an example, though it is not my own.  

Do we achieve this with a "thinner" glaze or one that is transparent ?  Usually we do not want the clay to show through a glaze, but for some effects, such as stamps etc, this is a desired effect.

Thought i would try a Mastering Cone 6 base, and color it for tinting.  

appreciate any help., cp

Views: 1159

Attachments:

▶ Reply to This

Replies to This Discussion

I just noticed this post and am surprised there aren't lots of answers here! Perhaps you've already tested some glazes and discovered what works for you but if you haven't I'd suggest glazes that move some so that there will be a flow over the design allowing some "break" to show. If you were referring to Mastering Cone 6, glossy base 1, I'm sure you'll find it works well. It is one of my staple glazes especially for functional ware, and it breaks nicely. 

Here's a sample of 12 glazes which have an interesting break in the Insight Live Glaze Database.

Many glazes with rutile will break because it's opaque when thick and translucent when thin.

Other glazes slow cool differently where thick or thin. We're currently using a 60 degree F slow-cool between 1,800F and 1,500 F.

Tests tiles are helpful because many glazes depend upon the thickness of the glaze application, with no break when the glaze is applied too thick or too thin.

Blue Matte Jayne Schatz

Busch Nutmeg

Clear Base Blue plus 10% 3269 Frit

Costello Carbonate Jayne Schatz

Floating Green

Frogskin is a uniform brown when applied too thin

Gartside Gloss (Peacock variation) shows the thick vs thin rutile

Lynn's Glossy Grey Green - uses titanium dioxide rather than rutile (titanium dioxide ore)

Magruder Red with 10% 3134 Frit

Magruder Red with 10% 5301 Frit

Morty's Green

White Bird - also a rutile dependent break

.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service