In January of 2018 I will be teaching an online glaze making course. I will be teaching course participants how to make and fire Ian Currie grid glazes. A grid glaze is a way to generate 35 glaze variations from a single glaze recipe. If you are interested in learning what this course is going to be about you can join my Ian Currie Grid Glaze group at this link.
https://www.facebook.com/groups/141620126569956/
~ John Post

Views: 839

Attachments:

Reply to This

Replies to This Discussion

John.

I started doing currie grids because of some of the tiles I saw on your website. I have been doing them for a year or so now and I find them most excellent. I would like to join any group discussion on grids or glazes, but seeing that it is facebook I will not be able to. Is there not another place you could host the discussion for those of us who don't use facebook? 

If not no worries, just thought I would ask.

Joseph

I moved your picture inline of the article for graphic impact. If this is an issue I will set it back on your objection.

Hi Joseph,


The reason I am running this course on Facebook is because of its universality. Billions of people use it and know how to upload photos and share content on it. So instead of course participants having to figure out how to use a new interface, they can simply work within a framework that they already know.

John

Joseph Fireborn said:

John.

I started doing currie grids because of some of the tiles I saw on your website. I have been doing them for a year or so now and I find them most excellent. I would like to join any group discussion on grids or glazes, but seeing that it is facebook I will not be able to. Is there not another place you could host the discussion for those of us who don't use facebook? 

If not no worries, just thought I would ask.

Joseph

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014