When a recipe calls for rutile, which should be used? Thank you

Views: 865

Reply to This

Replies to This Discussion

Light rutile is dark rutile which is already fired to eliminate off-gassing from components which are not rutile, so you want light rutile. - https://digitalfire.com/4sight/material/rutile_1204.html

Rutile, being a natural ore, is one of the most frustrating ceramic ingredients I've used. Every time we buy a new 10 pound bag of rutile, the rutile glaze looks quite different from every bag of rutile we've used previously - which can be good or bad.

^^

I recently bought some titanium from a different supplier. I swear I got rutile instead. I won't be buying titanium there again. I find it to be incredibly frustrating as well. Every time I try a different supplier for titanium it's the same issue as you describe. Completely DIFFERENT glaze results, be it color or texture or anything.

I immediately labeled the jar of 5# "bad titanium maybe rutile." I then ordered 5# from my online supplier who has the better stuff. 

BLEH! I don't like rutile at all. I found it's way to unreliable. I much prefer titanium, and even it has problems.

Catherine,

I love rutile! If the recipe just says rutile, I've used regular rutile; it hasn't presented a problem so far. The studio where I work has both, but at home, I plan to run some through a bisque fire if I need light rutile. 

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service