So I have a curious question for all you cone 6 firers out there. I recently refired a few pots and the glaze was completely free of microdimples. I have really good surfaces on most of my glossy glazes but there are always really tiny dimples, you can't even see them unless you hold the pot about  8 inches from your eyes. However on these refired pots, they had no microdimples!

So it got me thinking about trying something I have never tired before. 

Firing to cone 6, dropping to 1940F then firing to cone 6 again. Of course the glaze I am using doesn't move at all, so I am not worried about it running off the pots. I am just curious if anyone has tried this method before or something similar. I am super particular about bad surfaces on my glossy glazes, if this solved it I would be happy to do it as refiring all my pots for a better surface seems a bit crazy.

I was looking at commercial ware at a local shop and I noticed almost all of their pots when held up close have microdimples as well, so maybe I shouldn't worry about it too much, but I just can't help to try something new to see if it works.

Anyone? Any Ideas? Comments? 

Views: 996

▶ Reply to This

Replies to This Discussion

Just an update. I ended up doing a grid test of this glaze and I was able to achieve a perfect surface by finding a glaze with slightly more flux. It is still within limits and is absolutely stunning. Here is a close up. So instead of trying to use my schedule to fix problems, I just did the right thing and fixed the glaze. yay!

Great news! I thought maybe playing with the flux would give you the surface you sought. I am glad to hear it worked. Testing can be tedious but it usually pays off. Thanks for the update.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service