Hi all - I did not schedule a slow cooling cycle when I fired the kiln, but decided after it had reach temp that I wanted to try it.  Is there a way you know of to program this way?  I was planning 500f/h to 1900, then 150F/h to 1400, but when I press start it thinks the program is finished.  Thoughts?

Views: 357

▶ Reply to This

Replies to This Discussion

Stop the kiln. Reprogram quickly adding your new ramps/holds. Start the kiln. Skip ramps and holds already passed. -- How to do that depends on what controller you have, and if it allows you to manually skip segments. Watch out for adding more segments than the controller allows.

You could hurry and do a 3 segment program.  The first segment would be a "9999" ramp back to your top temp and then the other 2 segments you have mentioned.  Your kiln should ramp back up to the top temp & then do the downward ramps.  jhp

Jeff, good idea - that sounds like it might work.  Thank you!  I will try it.

George - it doesn't let me do anything, because it immediately shuts off, thinking the firing is complete.

Providing your kiln hasn't dropped too far down....  jhp

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service