I'm new to ceramics - very new.  So I bought some clay that's going to bisque fire white and assembled a slab birdhouse.  I'm certainly not going to brag about it but it was an enjoyable first effort and I learned a lot so I'll use up the rest of the 25lb of clay and make some more bird houses. My approach to decoration was going to be to use underglaze and cover with a coat of clear. 

But then I read that if I try to brush on the clear, that it would re-hydrate the underglaze and I would have a mess.  Is there a method I should follow to prevent this?  Or, is my approach a bad idea altogether?

Thanks for your comments.

Views: 158

▶ Reply to This

Replies to This Discussion

Most of the underglazes I have played with have enough binders in them, that if you let them dry, they should not come off with properly applied clear glaze. Your clear should be brushed on in one direction, with a high capacity brush (hake or similar) always laying down material, and not working it back and forth.

The big problem with underglazes is getting them thick enough that they don't go transparent as a thin layer is dissolved into the glaze melt. 2-3 coats of underglaze should resist the attack of the glaze melt.

Thanks George.  I'll give it a shot.  I just built another bird house today.  I think I'm going to like this as a retirement gig.  Tomorrow, I'm going to start on a kick wheel.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service