From a 1959 home, this glaze is satin, and the glaze seems to randomly "bunch up" and show a darker under-color.

I have seen the same kind of glaze in a light grey with a dark grey under color.

I imagine some chemical ingredient increases surface tension, since the glaze really does pile up a bit on the borders of the crackle look. I wonder if lead was required in the formulation. I cannot tell if a separate underglaze was applied to create the contrasting color, or if it is just a part of the glaze itself.

At least one tile in this glaze was factory made in Italy.

Any insights or guesses would be welcomed!

Hi Nancy,

    It looks like a glaze with a lot of "float" in it.  I bought some glaze from Bath Potters that is a ringer for it called Blue Speckle.  Problem is it was on close out and they don't make it any more.  When I asked why, I kind of got the feeling that it may have had lead in it. A lot of the Amaco Potter's Choice glazes have the "float" in them, but they have to be put on thick.  The "float" is just crystals floating on the clear glass matrix.  Cooling has a lot to do with it forming. Western Glazes has a few that look like that but I think the ones that do are earthenware glazes.  jhp

Very good ideas to pursue! I am very open to lower fire options so appreciate the tips.

I've had fun playing with Assad Black which creates a matte, except in areas where the glaze is thicker.

It's colored with 4.2% copper carbonate in a nepheline syentite glaze.

A layer of Assad Black, then coated again and refired.  When thick it crawls.

A thinner layer of Assad Black on the interior. Over a titanium dioxide wash on the exterior.

I see what you mean. It does create a very intriguing surface.

Norm Stuart said:

I've had fun playing with Assad Black which creates a matte, except in areas where the glaze is thicker.

It's colored with 4.2% copper carbonate in a nepheline syentite glaze.

A layer of Assad Black, then coated again and refired. When thick it crawls.

A thinner layer of Assad Black on the interior. Over a titanium dioxide wash on the exterior.

After more research and reflection, your magic word "floating" led me also to the Digitalfire database on this type of glaze and its evolution and components. Thank you again.

Jeff Poulter said:

Hi Nancy,

    It looks like a glaze with a lot of "float" in it.  I bought some glaze from Bath Potters that is a ringer for it called Blue Speckle.  Problem is it was on close out and they don't make it any more.  When I asked why, I kind of got the feeling that it may have had lead in it. A lot of the Amaco Potter's Choice glazes have the "float" in them, but they have to be put on thick.  The "float" is just crystals floating on the clear glass matrix.  Cooling has a lot to do with it forming. Western Glazes has a few that look like that but I think the ones that do are earthenware glazes.  jhp

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service