So this is the first time I have seen this error.  The manual says that the temperature was decreasing in the last ramp of a cone fire program. It says possibly the kiln was shut off by the sitter if it is using a wall mount controller.  This doesn't apply to my situation.  I peeked in and the glazes were definitely not matured & I didn't see any obvious signs of a catastrophic failure.  Anybody have experience with this code & can point me in the right direction?

Views: 421

▶ Reply to This

Replies to This Discussion

I'd bet money you're going to find failed heating elements or less likely a failed relay.

This type of error on our Cress customized Bartlett controller is reduced to

"Error 1" =  Ramp segment rises < 12 F per hour for 22.5 minutes.

In our over-powered kiln we don't err out until the second or third element fails, depending on which coils they are.

As you know we just stick paper under each coil and fire for 10 minutes as a diagnostic.

I'm betting on relays as the elements are in really good shape.  Lately the relays haven'y been sounding right.  Either way it's going to cost me money!  jhp

So one of the relays was bad, but I am replacing both.  I wanted to replace the relays as they went out with SSR's.  I have the SSR's, fins & fans but I would have to modify the box & wiring and I don't have time to do that now.  Anyways, everybody wanted between $25 to $27 for the relays , but I found them at Newark for $9.90/each so I am stocking up.  Just thought I would share in case anybody else wants to stock up, too.  jhp

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service