I was mixing a batch of Steven Hill's Strontium Crystal Magic (warm) and was tired and in a hurry when I got to the Bentonite.  I read across the line wrong and added 2.8 instead of 2.3% bentonite (2.8 is the amount of yellow iron oxide.)

I understand that the effects of bentonite on flocculation reach an optimum peak and then fall off again as the percentage increases.  And I've also read that even messier things may happen.  What I don't know is the breadth of the curve of optimum effect. 

If I need to increase everything else to reestablish percentages I can do that, but I'd rather not if the effect is negligible.

I've just finished a "booth", have a compressor and a sprayer of sorts and am anxious to try spraying glazes.

Here is a humorous article that I wrote elsewhere with pictures of the "booth".

Views: 245

Reply to This

Replies to This Discussion

Im not sure on the answer for the bentonite.. If it was me, I would not make any adjustments, just knowing that the glaze will be a little thicker. I imagine.  Now that spray booth looks like something I would make.  Straight to the point, and easy!  Now tell us after you use it, does it do the job?

J

Chemistry wise there's such a small difference between 2.3% and 2.8%, unless it something like cobalt oxide.

Bentonite used to seal the bottom of ponds and used as a drilling mud additive is rather weak stuff, compared to brand name Veegum or Bentones which have perhaps 10 fold or 15 fold the suspending effect.

I always got the impression that 2.3% Veegum was quite a bit too much with strontium crystal magic. But I've never seen Steven Hill mix it up in person, so I really have no idea.  But when I've run across the occasional recipe calling for 4.5% bentonite I've found it safe to assume they didn't use a very powerful bentonite.

I've only noticed a difference when a recipe calls for a very small amount of clay and I've used bentonite instead. In those cases there's a much higher ratio of silica to alumina in bentonites, say 3 to 1, than there is in clays, which are closer to 1 to  1.

I will give a follow-up on both the glaze and the booth.  It will be interesting to see how long it holds up, and whether my exhaust system works.

juli long said:

Im not sure on the answer for the bentonite.. If it was me, I would not make any adjustments, just knowing that the glaze will be a little thicker. I imagine.  Now that spray booth looks like something I would make.  Straight to the point, and easy!  Now tell us after you use it, does it do the job?

J

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014