Does anyone have experience with their kilns over firing? It seems that most struggle with under firing.

Views: 470

▶ Reply to This

Replies to This Discussion

Our kiln with a Bartlett V6-CF electronic controller uniformly fires exactly one witness cone too hot, whether firing to Cone 016, 04 or 6.  Inexplicable, but this is very easy to adapt to by simply choosing one cone cooler than we need.

Even with this odd quirk, I highly recommend the $430 Bartlett V6-CF electronic controller to replace any kiln-sitter.  It works like a microwave oven . . .

Cone-Fire 5, Medium speed, 3 hour pre-heat, Add slow-cooling program, Start. 

It takes less than 30 seconds to program a firing.

http://www.clay-king.com/kilns/olympic_kilns/electro_sitter.html

Our Cress E-32 is amazingly even - a handful of witness cones spread through-out the kiln end up looking nearly identical.  Larger kilns can vary in heat work from one shelf to another and from the center of a shelf to the edges, unless the firing is done slower.

I would never use a kiln sitter again. With a kiln-sitter, if the little matchstick cone melts partially onto the metal support arms you get an over-fire, with lots of ways to under-fire as well. And the kiln-sitter we used was warped from years of heating and cooling, making even less reliable.

The only change we have made to the controller system over the past five years was replacing the Type-K Ni-Cad thermocouple when it wore out after a couple of years with a Type-S platinum thermocouple, which lasts longer and is more accurate.

Type-K thermocouples cost $46 and are accurate to +/- 10 F.  As this type of thermocouple ages their accuracy can "drift" in one direction or another as the metal crystallizes. Even with this known inaccuracy, in our experience, kiln firings were far more correct than they used to be using a kiln-sitter.

The Type-S platinum thermocouple, apart from costing $180 instead of $46, doesn't drift in accuracy as it ages, and is allegedly accurate to +/- 2 degrees. We've had no complaints. You have to push a few buttons to change the controller for the different thermocouple type.

How accurate is +/-10 degrees F?

The difference between Cone 1 and Cone 2 is only 9 degrees F, whereas the difference between Cone 5 and 6 is 65 degrees F.  Of course the kiln controller is accumulating the heat readings every 30 seconds or so to determine the total heat work done using an "area under the curve" integral.  But the accuracy of each individual temperature reading is what determines the length of each firing.

After initial testing following our installation of the Type-S thermocouple we rarely use witness cones. We no longer need them.

The 3-Key kiln controller on the left costs $100 less ($330). People I know who've purchased one have always regretted saving $100 to end up using this much less capable controller.  You want the V6-CF.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service