I've recently done some experimenting with lidded containers and have got a gallery/lid method I'm happy with. I'm wondering about glazing them.

When doing these is the contact surface glaze-glaze, glaze-unglazed, or unglazed-unglazed I'm thinking for practical considerations for functional pots that will store foodstuffs.

Views: 639

Reply to This

Replies to This Discussion

Patricia Bridges is the best person to get advice on functional wares from...

Hi Tom. If you glaze the lids and the pot  you can't have two glazed surfaces together while they are being fired unless your goal is to make time capsules. They will fuse together forever. If you are firing your pot with the lid setting in place then both surfaces need to be unglazed and you need to account for the fact that some glazes run when they melt. You can glaze a pot so the whole surface is glazed, but you will have to glaze the lid by itself and use the unglazed foot of the lid to keep the glaze off your shelves. Then you have to be careful that the glaze on the inside rim of the pot is not to thick or it will keep the lid from falling into place. Getting lids to work can be challenging. Maybe someone else has some more useful advise. Happy Firing  

Me again Tom. I was looking at some gallery type lids, I said the "foot of the lid" to hold the lid up off your shelf. I see it is called a flange not a foot, my bad. I was taught that is best to fire your lids on your pots because that way they warp the same.

Thanks for the reply kabe, I was going to bisque fire them together. And was planning to glaze fire separately, I hadn't considered doing the glaze fire in situ but it would save some kiln space I suppose so I might experiment with that!

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service