hello,

I'm a new potter who plans to make my own glazes following recipes I find online.  I'm firing them in my home studio at cone 6 in my electric kiln.

I love the Wright's Water Base Blue glaze I found in one of the Ceramics Art issues, but have trouble making this glaze adhere to the bisque piece before firing.  I have not had this problem with any of the other glazes I have made.  Here is the recipe I followed:

Copper carbonate 5%

Lithium carbonate 3%

Strontium carbonate 9%

Frit 3110 59%

Edgar Plastic Kaolin  12%

Flint 17%

Add: Bentonite 2%

Is there anything you can suggest I add to this already mixed glaze (I made up a large batch!).

Someone suggested coating my pieces with karo syrup to help it adhere, but didn't work.  I've tried the brushing medium, but again no success.  Would appreciate any advise on salvaging this glaze, and in addition, what is wrong with this recipe.

thank you,

Rita

Views: 2709

Reply to This

Replies to This Discussion

The price of Bentone-EW is comparable at $11.50 for one pound, compared with Axner's price of $11.79 for VeeGum, or $10.99 for Macaloid.  But since this had to be shipped from Texas, rather than being included with our regular truck delivery from Laguna, there was an extra  $9.11 for shipping.

Low quality bentonite costs something like $1.50 a pound.  We have a very old 50 pound bag from when our studio was at a different location - and I don't really know what to do with it.  Suspending glazes with it changes their look significantly.  Most low-quality bentonite is used as a component of drilling mud, or used for sealing reservoirs.


Nadine Mercader said:

Norm, How does the Bentone W compare in price to bentonite?


Norm Stuart said:

Juli -- The sediments at the bottom of glaze buckets are an essential part of the glaze.  With Cone 6 glazes this sediment in primarily the frit (the ground glass which makes the other ingredients melt properly).


If your glaze doesn't have enough clay, I definitely recommend Bentone-EW which I bought from Trinity Ceramics in Texas. US Pigment will be stocking this item soon, and may already have it.  If a glaze requires 1.5% bentonite to suspend, you use only 0.1% Bentone-EW and it mixes well just adding it to the glaze or water - quite unlike common bentonite.

Thank you Norm, I have not been happy with the bentonite that I have, I will ditch it and try the Bentone EW.

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service