I'm confused by what I'm reading in various places.  I have a glaze recipe that calls for Kaolin.  Are there any acceptable substitute?  The recipe I'm working on is Cream breaking Rust.

Views: 970

Reply to This

Replies to This Discussion

I think you will find the Digitalfire Materials Database very useful.

http://digitalfire.com/4sight/material/index.html

Kaolin is a hydrated alumina-silicate composed of 40.21% alumina and 47.29% silica, and 12.5% water.  In theory you could use alumina hydrate and silica in place of kaolin, but kaolin or other clay is usually the primary ingredient which suspends the glaze. 

More to the point, 50 pounds of kaolin costs only $16, comparable to the price of silica.  Alumina hydrate is five times more costly.

http://digitalfire.com/4sight/material/kaolin_925.html

Each molecule of Kaolin (Al2O3 · 2SiO2 · 2H2O)  loses the two water molecules, 12.5% of its weight, between the temperature of 986 F and 1,166 F,  forming metakaolin.  Most kiln firing programs slow during part of this temperature range to allow time for this super-heated steam to escape.

Kaolin, originally sourced and used in Kao-Ling China, has roughly 60% more alumina than other clays.  Not surprisingly it's also called China Clay.  The particle size of kaolin is much larger than clays so kaolin is not at all plastic.  In America the most commonly used kaolin has the brand name of EPK (Edgar Plastic Kaolin) which is mined in Edgar, Florida.  http://digitalfire.com/4sight/material/ep_kaolin_291.html

http://digitalfire.com/4sight/material/ball_clay_80.html

Looking at the two reference pages above for EPK and Ball Clay, you can see you could substitute any white clay for kaolin, but the resulting glaze will be somewhat different.

English Kaolin has more flux and titanium dioxide so fires whiter.  http://digitalfire.com/4sight/material/english_kaolin_289.html

Chinese porcelain was originally made from a mixture of Kaolin and a feldspar called Petunse.  China Stone is a feldspar similar to Petunse which is found in many other locations around the world.  http://digitalfire.com/4sight/material/petunse_1116.html

Wow Norm, thanks for the indepth response.  I did find my kaolin.  But your response left me thinking about a couple of ways to alter and test a few glazes. 

On another topic.  Do you know where I can find info explaining how the slow cooling in electric cone 6 changes glazes.  I have never read any info explaining why this works, only that it does.

Thanks again, chantay

If you cool glass quickly, it freezes into a random structure, analogous to gassy lava spewed from a volcano.

If you cool glass slowly, crystals of various types have time to form. The formation of an orderly structure takes time.  Crystals on the surface of the glass refract the light making it look more matte and less shiny.  Depending on the chemistry of the glaze you grow different crystals of of various types of minerals or gems.

We are limited with our kilns by the fact that they work at atmospheric pressure.  Some crystalline formations, like diamonds, require extreme pressure in addition to slow-cooling.

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service