I had posted a recipe and test results last month for a glaze called Dave's Blue.  Today I went to mix up another batch.  I realized that I used Cobalt Carbonate instead of the listed Cobalt Oxide.  The glaze looked good and fired well.  I don't know enough about chemistry, but can anyone see a problem with this sub?  I don't even have Cobalt Oxide, $$, and plan to continue to use the recipe with the cobalt carbonate.

Views: 325

Reply to This

Replies to This Discussion

Cobalt oxide is about twice as strong as carb & tends to speckle more whereas the carb seems more uniform in color.  It depends on the recipe.  There are some that I only use oxide and others where I use carb.  If I have to sub, I usually use 1 1/2 to 2 times as much carb as oxide depending on the recipe.  The good thing is that a little cobalt, no matter what the form, goes a long ways!  jhp

Jeff hit it dead on.  I would like to see samples of the previous glaze and this new one.

I'm only making the glaze with the cobalt carbonate.  I don't have any cobalt oxide and it will be a month or so before I can get some. $$.  I will post test tiles after I fire this batch.  There is a pic on Insight live with the recipe. OK, found pic of previous test batch that used the cobalt carbonate.

Attachments:

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service