Potters & Sculptors - Making Rock from Mud
Tags:
are you coating the elements with ITC coating?
Hello all
First let me shy away from being an expert, I have a few years into it, and I maybe ahead of the curve, however reduction in electric kilns has been going on for, as long as the electric kiln.
I must say I loved reading Tim Eberhardt’s tails of his reduction trials.
( It’s a must read )
I will attest that every thing he wrote about is true, I fail for years trying each and every thing he did with the same results ( burned up kilns )
There are ways we all have heard about. Using some form of combustible and introducing it into the kiln at a certain temperature to get some level of reduction.
These techniques must be taught one on one. There are many dangers primarily to ones life not only to the kiln.
As to ITC coatings, I use the ITC coating for brick, mainly I like the appearance it gives, I also think it seals up some small fracture in the brick.
As to coating the elements it is not worth the effort, you will not see any benefit from it. To withstand the effects of the reduction atmosphere on the elements you need thick gauge elements and the right wire like Kanthal A-1 or APM and you need to re-oxidize the elements after each reduction firing. ( There is no free lunch )
Like any technique, and this one in particular there is a lot to learn.
One mistake could mean $ thousand of dollars to repair the kiln. Or the worst of all, yours or someone else’s death from Carbon Monoxide.
§terry
Hey George. I thought I'd weigh in here. I've been firing ^10 electric reduction for almost 8 years as my primary means of firing. As with any other means of firing, it comes with its own set of problems and challenges........but it is a very reliable and efficient means of firing. AND, when done properly yields results that are excellent. I made a little video a few days ago that documents my most recent firing. Also, you might want to check out my latest post at my blog.
Blog: www.theduckdroppings.blogspot.com
Take care,
Nick Friedman
The Duckpond Pottery
Brevard, North Carolina
great video!
really informative, stuff I have wondered about and now understand!
thanks Nick!!
Sandy Miller
The Fallonator TM System; Is a complete system, anyone using a Fallonator TM product, will state "I use Fallonator TM Product" as part of a contractual agreement.
"Nicholas Friedman" is not a customer of Fallonator Products TM.
We must assume his statements reflect his knowledge base on; his use of his equipment, and that this assembly of miscellaneous components contains zero components obtained through Fallonator Products TM.
The Fallonator TM Gas-Add-On-Kit
This is a system to add the ability to add reduction atmosphere to an existing electric kiln.
We supply a 100% System.
No modifications are made to the kiln.
No holes, nothing, other than the removal of the top most peephole plug and the bottom most peephole plug.
No adjustments to port openings.
No primary air adjustments.
No secondary air adjustments.
We supply the fuel in one pound bottles.
We supply locale suppliers for you to purchase replacement fuel.
As low as $2.99 per pound.
We do not offer a system that uses 20 pound propane barbeque tanks.
We supply replacement O2 sensors for $70.00, New “not rebuilt” “not repaired”
We do not make our O2 sensor. Our O2 sensors are made by BOSH a leader in the industry of Atmospheric Sensor.
Mr. Nicholas
I must commend you on your efforts. I have praise and commendations for you.
Your are, where I started so many years ago.
The time and commitment to get past the continuous element failure, show you have perseverance.
To acquire the components, assemble, test, and learn how to control the reduction, must have been a proud moment for you.
The kiln opening after your first successful reduction must have been an eye opener for you, it was a moment in time I will not forget.
terry
Ms. Sandy
Please do not rip your kiln apart, you don’t live so far away that you don’t have a phone.
Contact me through Fallonator.com
A little preparation will make the difference between you being able to reassemble the kiln, and Humpdy Dumpdy fell off the wall.
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014