Hi, I have been following this forum for months and have finally found the courage to do my first posting. I am a ceramics hobbyist for around 3 years and over the last year have shifted my focus to cone 6 glazes.

The picture below was taken from an exhibition. The 'sugar powder' is very fine and I suspect should not be due to silicone carbide additive. Has anyone ever come across such a glaze recipe ? 

Views: 375

Attachments:

▶ Reply to This

Replies to This Discussion

Interesting effect. Like snow fall. I would test the whitest clay I can find and try adding  a flux such as frit 3124 in a line blend experiment.

95% clay 5% frit

90% clay 10% frit

85 : 15

80 : 20

75 : 25

70 : 30

Then sprinkle each of the dry powders on test tiles and fire.

One of those will sinter enough to hold the particles together, but won't melt into a traditional glaze.

You can then retest in smaller percentage steps around the best tile from your first group to get the best combination of look, hardness, and attachment to the pot.

I put the image directly into your posting so people don't have to open it to see.

Thanks George..will try out the tests. A newbie question : only the forum adminstrator can 'put the image directly into your posting' ? If not, I would like to to so myself in future. 

Any member can add inline pictures to their discussion or blog postings. See the Pictures section of the "New User Guide"

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service