Olga Biff's Discussions

Buying my first kiln

Started Feb 20, 2020 0 Replies

Hello all,I will be buying my first kiln ever in a few months and I was wondering if I could get some advice.  I want to fire at cone 6. My choice is between a Rodhe Ecotop 60LS (III) Kw5,0 and a…Continue

Tags: kiln

Bisque cycle for heavily grogged clay

Started Jan 17, 2020 0 Replies

Hello,I usually bisque my clay at 980C. I am thinking of changing to a heavy grog clay for bigger sculptural pieces. So, the higher the grog content in the clay the hotter the bisque temperature?Than…Continue

Wash Application

Started this discussion. Last reply by Kathleen Scott Feb 2, 2020. 5 Replies

Hi!How do I apply washes to enhance the look of a glaze? Could you recommend any good online tutorial or have any tips to share?For what I have read this world be a possible process:·Bisque fire the…Continue

Tags: application, oxide, wash

 

Olga Biff's Page

Latest Activity

Vanessa Herbert left a comment for Olga Biff
"Hello, How is everything with you, my name is Venessa Herbert, I picked interest in you after going through your short profile and demanding it be necessary to write to you immediately. I have something very important to disclose to you concerning…"
Aug 26, 2024
Olga Biff posted a discussion

Buying my first kiln

Hello all,I will be buying my first kiln ever in a few months and I was wondering if I could get some advice.  I want to fire at cone 6. My choice is between a Rodhe Ecotop 60LS (III) Kw5,0 and a Nabertherm Top 80 (III) Kw 5,5, they fit my price range. I am writing because I have read somewhere that a Rodhe Ecotop 60LS don't perform well for firing regularly high temperature glazes.  I find the controller of the Nabertherm series a bit confusing, the Rodhe TC304 is much simpler to me.  What…See More
Feb 20, 2020
Kathleen Scott replied to Olga Biff's discussion Wash Application
"I do a lot of washes in my work. I have this recipe I learned in university. It is my go to recipe. Kingsmill Wash - 33% red iron oxide, 33% Alberta slip, 33% Bannard clay Sometimes clear glazes can absorb the iron in varying degrees. The cup shown…"
Feb 2, 2020
Olga Biff posted a discussion

Bisque cycle for heavily grogged clay

Hello,I usually bisque my clay at 980C. I am thinking of changing to a heavy grog clay for bigger sculptural pieces. So, the higher the grog content in the clay the hotter the bisque temperature?Than you!See More
Jan 17, 2020
Olga Biff replied to Olga Biff's discussion Wash Application
"Thank you."
Jan 17, 2020
Olga Biff replied to Olga Biff's discussion Wash Application
"Thank you Donna!"
Jan 17, 2020
Donna Kat replied to Olga Biff's discussion Wash Application
"On bisque ware, under the glaze you can wipe away to give greater depth and variance in the color. You may risk crawling but I have not seen it. Over the glaze you can dilute it and use as you would water color painting (same for under as well). You…"
Dec 28, 2019
George Lewter replied to Olga Biff's discussion Wash Application
"Our member Carl Cructhfield probably uses stains and oxide washes more regularly than most of us. Check his work.  You can download a free booklet from ceramic arts network daily on stains and washes. Go…"
Dec 12, 2019
Olga Biff posted a discussion

Wash Application

Hi!How do I apply washes to enhance the look of a glaze? Could you recommend any good online tutorial or have any tips to share?For what I have read this world be a possible process:·Bisque fire the piece·Apply the oxide wash with a brush or sponge and wipe off excess·Let dry one day (or longer if needed)·Glaze as usualCould also be done on top of the glaze? Would not the glaze be "washed away"?Thank you so much!See More
Nov 29, 2019
Olga Biff is now a member of Electric Mid&Hi Fired Ceramics
Nov 28, 2019

Profile Information

What is your experience with ceramics in general. (Long answer encouraged)
Good handbuilder beginner in glaze formulation
What is your current involvement with electric fired ceramics? (long answer encouraged)
Practicing daily
All our content is viewable by the public. Why do you want to be a member, when you can already see everything as a non-member?
To share knowledge
Where do you work on your ceramics projects?
co-op
How did you find this network?
search engine

Comment Wall (1 comment)

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

At 11:39pm on August 26, 2024, Vanessa Herbert said…

Hello,

How is everything with you, my name is Venessa Herbert, I picked interest in you after going through your short profile and demanding it be necessary to write to you immediately. I have something very important to disclose to you concerning your surname that's to say your last name .since it's a public site.Could you please get back to me on: (

vanessaherbert1872@gmail.com

) for more details.

Regards.

Venessa.

 
 
 

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service