Potters & Sculptors - Making Rock from Mud
Started this discussion. Last reply by Darthe Hues Apr 14, 2012. 5 Replies 0 Likes
The first four glazes in the front row (left to right), which were on the top shelf of the…Continue
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
Switch to the Mobile Optimized View
© 2026 Created by Andrea Wolf.
Powered by
Comment Wall (6 comments)
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics
Good day,
I am Ronald Morris, I saw your profile and I decided to contact you immediately. Can you get back to me on my email (ronmorri01@gmail.com) for full details.
Regards.
Good day,
I am RonaId Morris, I saw your profile and I decided to contact you immediately. Can you get back to me on my email (ronmorri01@gmail.com) for full details.
Regards.
I tried to email you a mentor invitation to the 2017 Alaska Claycation. Got a bounce back notification that you - - - -
June, I posted the results on my blog page too. Dont know why you cant see them on this site. Maybe you are missing a minor update with your computer that would allow you to see them. ;Active X; or similar??? Anyway, here is my blog address.
http://janwallacepottery.blogspot.com
Welcome, June!
I've admired your work for some time. A link to your cone 6 glaze tests has been on this site for a couple of years now.
Welcome June...Your glaze test pages on your website are a fantastic resource...well done. Your new soda work is looking mighty fine as well. Best Wishes, Dale