June Perry's Discussions (39)

Discussions Replied To (17) Replies Latest Activity

"Here's a copy of that nutmeg glaze with the white satin over it as an accent. It's…"

June Perry replied Jun 6, 2016 to Getting a soda ash fired look with commercial glaze?

8 Jun 8, 2016
Reply by Pat

"Why not just make up a glaze. Here's a link to the nutmeg and other glaze which give…"

June Perry replied Jun 6, 2016 to Getting a soda ash fired look with commercial glaze?

8 Jun 8, 2016
Reply by Pat

"Since a picture is worth a thousand words, that 2nd tile from the left is the Carlt…"

June Perry replied Feb 6, 2013 to What is this glaze?

32 Nov 2, 2015
Reply by Brenda Outram

"Here's the late Ian Currie's recipe for a cone 6 matt glaze which mimics a tradition…"

June Perry replied Feb 6, 2013 to What is this glaze?

32 Nov 2, 2015
Reply by Brenda Outram

"Replacing the potspar with Neph sy will affect the firing range, because the Neph Sy…"

June Perry replied Feb 5, 2013 to What is this glaze?

32 Nov 2, 2015
Reply by Brenda Outram

"George, the results sheet I use for assessing tests has some of the following inform…"

June Perry replied Jan 20, 2013 to Online Glaze Recipe Database Project is Now Under Way

15 Jan 20, 2013
Reply by June Perry

"It looks like a typical copper, high barium carbonate matt. June "

June Perry replied Jan 20, 2013 to What is this glaze?

32 Nov 2, 2015
Reply by Brenda Outram

"Evelyn, check with your supplier. I suspect that if they only sell one type, that it…"

June Perry replied Jan 20, 2013 to Dark rutile v Rutile

12 Apr 17, 2013
Reply by Norm Stuart

Stars

"Randy, if you just copy and paste the photo into a program like Paint Shop Pro, you…"

June Perry replied Nov 29, 2011 to CORRECTED LIST AND NEW PHOTO OF CONE 6 TESTS

5 Apr 14, 2012
Reply by Darthe Hues

"I believe the dark rutile has a higher iron content.   If you're looking for a yello…"

June Perry replied Jul 20, 2011 to Dark rutile v Rutile

12 Apr 17, 2013
Reply by Norm Stuart

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service