I'd suggest refiring the green vase.
With a digital controller we always add a 20 minute hold after the controller indicates Cone 6 heat-work has been done. While in theory I think this accumulates a Cone 6.5, the reason we do it is to allow glaze reactions to finish and lay down. This may be more a problem for our kiln as it can achieve the final climb to 2,232 or so very quickly.
If your "speckles" are bubbles or pin-holing, a hold at temperature usually cures this. For us the exceptions which are not cured by a hold have been porous cone 10 clays fired at cone 6 with a reactive glaze which have penetrated deep into the clay body, or the rare occasion where the glaze reacts chemically with the clay. When this happens I have the ware refired to help understand what's happening. Some of these rare interactions continue into the third Cone 6 firing.
Your "speckles" can also be crystallizations, which we frequently see in our glazes doing a 6 hour slow-cool between 1,800 F and 1,500 F.
Do you think the speckles on the green one are because it was underfired?
I think I under-fired a bit also. ^6 barely bent. The glossy black wasn't very glossy.
It amuses me to watch some people spend a lot of time on some piece then immediately slather on some glaze without first firing it on a test tile of the clay they're using.
Most glazes take on a variety of looks depending on which clay they're used on.
ha ha, I know what you mean , the frogskin turned out terrible for me as well. I had such high hopes for it!
Nope, I wanted to make sure that the glazes worked. I'm glad I waited. The frogskin turned out terrible. I liked the Honey Amber, Rowes brown, Strong Celadon and Fat Cream though.
did you get this glazed in your last load?
Please post pics when you finish!!
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2025 Created by Andrea Wolf.
Powered by
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics