Potters & Sculptors - Making Rock from Mud
Comment
This is Kathy's test tile. This is what it should look like. I have several pots with it on my page but they are all layered with other glazes but you can still see the "frogskin". jhp
Hi Juli
Is that on a buff clay? I have never seen Frogskin look like that. I have used it on white, brown, red and porcelain but have never seen it look like that. It's almost like there is no copper or titanium dioxide in it. Mine has always come out very similar to Kathy's test tile. Even when layered with other glazes, it imparts its "frogskin" character. jhp
Jeff
The green is smooth. I don't mind the speckles (crystals?) but had no idea what they are. Thanks for the insight.
I always do a hold to let everything equalize at the top end. It also helps everything settle down and smooth out if the glaze has matured. of course it doesn't hurt to do a slow ramp back down for a little ways either. jhp
I'll post a frogskin tomorrow. Yuck
if that green is smooth and not pinholed or bumpy, I would say those are crystals. jhp
Norm
Thanks so much for the sharing your knowledge. I will try refining with a hold.
Is it generally better to overfire a touch rather than underfire a little?
I would really like to see other people's tests of Frogskin, as it has always been a very beautiful glaze for me.
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014