Potters & Sculptors - Making Rock from Mud
Comment
Hi Trish,
Yours came out pretty close, sorry you don't like it. It could have gone a hair higher for the melt and a slow cool definitely gives more crystals but you can tell it's Frogskin. jhp
Not all frogs are the same.
Frogskin seems to look completely different on each different type of clay.
Ceramics really does require controlling a huge number of factors.
Jeff,
Since I just made only 200 grams, I did not sieve... Usually I sieve glazes that have a lot of one colorant, or one that has not been used for a while. Well, maybe, I sieve most large batches, not smaller test batches. 100-500 gram.
I can't imagine those subs having that dramatic of an effect on the recipe. Are you sieving the glaze? I'm a firm believer in the non-sieving as I think you can sieve a lot of character right out of the glaze. I have noticed when I spray this particular glaze that there is a little clumping going on, but nothing that won't go through the sprayer at 60 psi. jhp
Jeff,
I subbed the Custer with G200hp, and Gerstley Borate with Gilespie Borate, and upped the silica by +1.
I tested it over white universal slip, and you can see a tad bit more green, that on the test tile with just buff clay.
Just checking to make sure this is the recipe that you are using:
Custer Feldspar 22
Gerstley Borate 22
Neph Syen 22
Silica 26
Wollastonite 3
EPK 3
Titanium Diox 2
Red Iron Oxide 3
Copper Carb 4
Bentonite 2
This is the one I use that Kathy posted here on this site. jhp
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2026 Created by Andrea Wolf.
Powered by
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics