Comment by Norm Stuart on May 15, 2015 at 3:24pm

We had a ceramics instructor visit the last sale at our studio and one member asked her what she thought of his thrown work.  She provided some very thoughtful insights on how he could improve his technique and how these would improve each of the pieces he's made.

I don't think he's over the shock of it yet — says the chemist who's never really thrown anything himself on a wheel.

I watch videos like this one below, amazing to me, of a potter in Jingdezhen China trimming a porcelain pot, and wonder how long he's been doing this.

https://www.youtube.com/watch?v=o10UBL6oaIQ

A college ceramics professor had previously told me the, sometimes wafer-thin, porcelain from Jingdezhen has historically always been thrown too thick — then trimmed by people who were very specialized in trimming thrown pieces, and I can see that's the case in this video. The cost of recycling clay being insignificant.

The simple tool he uses, which he bends into a new shape with pliers for each new aspect of his trimming job, reminds me of this Chinese Proverb

"A bad workman always blames his tools."

一个坏的工人总是指责他的工具‎

Yīgè huài de gōngrén zǒng shì zhǐzé tā de gōngjù

And to think, virtually all of these porcelain factories in Jingdazhen went bankrupt around 1998 or so in the face of slip-cast work from Viet Nam and other sources.


Stars
Comment by Denice E. Demuth on May 15, 2015 at 11:53am

I know giving a critique on a forum can be touchy, but it was so close to being perfect I couldn't help myself.  It's too bad that they can't have an section where you can give critiques.  The problem is that a percentage of the population  isn't mature enough to give a proper critique or accept it.   It's nice to meet a mature person.   Denice

Comment by Trish Eckman on May 15, 2015 at 7:31am

Denice, I actually appreciate the critique! Thanks!


Stars
Comment by Denice E. Demuth on May 15, 2015 at 7:22am

I like the break you have just below the neck and also has a foot that helps balance it.  Think about a break or groove below the lip next time and this will tie into your other break.  This type of detail work and thinking in 3's was pounded into my head in college.  The glaze is also nice, I hope you don't mind a small critique.     Denice

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service