First attempt at carving and inlay. Need a lot of practice to develop the skill to apply this technique proficiently...

Materials:
G-Mix Cone 6 Clay
4% Cobalt Oxide in Trillium Cone 6 Porcelain Slip
MC6G Glossy Base 2 Glaze

Views: 135

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Jay Decker on July 6, 2015 at 10:26pm
Thanks Denice.

I'm a noob don't know what B Mix is. The G-Mix 6 is a cone 6 stoneware clay that I purchase from Georgies in Portland, OR. The only other clay I have used is a local earthware clay the guy who taught me what I know about pottery digs and uses in his studio. So, far I really like stoneware and the plasticity of the G-Mix 6 clay.

I'd love to learn more about the cutting tools that you are referring to. I used a broken long tweezers blade that I bent and filed into a hook shape with sharp edges to carve this. Have any photos or links regarding what works well for you?

Stars
Comment by Denice E. Demuth on July 6, 2015 at 6:35am

Nice start, is G-Mix similar to B Mix, B Mix might be easier to cut.  Nice sharp tools would help, I get some from the local ceramic store that has a set with different shapes and sizes a sixteenth to one quarter inch wide or they can be bought individually.    Denice

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service