Potters & Sculptors - Making Rock from Mud
wonderful golden colored plate with porcelain slip brushed around the rim to give contrasting views of the same glaze. the glaze is sprayed all over, then piece is fired to cone 6 electric. this one is about 14 inches in diameter
Tags:
Albums: new pieces 2015
Comment
Different transliterations but I've invested the spelling variations with a new meaning.
Generally all but one of the Cornwall Stone or oxidation recipes were Tenmoku, except for one. All of the older reduction recipes were Temmoku. So I changed the m to an n for the one recipe which didn't conform to the pattern.
Now it's a thing to do. if you want.
As far as I know the spellings are not intentionally to designate reduction or oxidation, they are just a couple of variations in trying to approximate a Japanese word. Similar to Nipon and Japan - Japan eventually became the accepted mispronunciation.
In our Insight-Live glaze database Temmoku are reduction glazes while Tenmoku are ^6 oxidation.
Juli - This is Digitalfire's Original Cornwall Stone recipe.
The original mine was depleted and the new mine has a different chemistry.
| 100.0% | Cornwall Stone Substitute - not a glaze | |
| 30.4% | Feldspar Custer Potash | |
| 29.3% | Silica | |
| 23.8% | Nepheline Syenite | |
| 12.9% | Kaolin | |
| 3.3% | Wollastonite | |
| 0.37% | Dolomite | |
| 0.3% | Strontium Carbonate | |
| 0.3% | Zinc Oxide |
The last two additions Strontium and Zinc are mine, to more faithfully recreate the Original Cornwal Stone chemistry.
Alisa Clausen calls the Tenmoku Gold recipe V's Tenmoku Gold. I have seen others call it Vee's Tenmoku Gold.
So I have renamed it Tenmoku Gold V's ^6.
https://www.flickr.com/photos/glazes/1085550860/in/set-7215760204
I have just added Tenmoku Gold V's w/o Cornwall Stone ^6 my initial "chemically identical recipe" without original Cornwall Stone. This includes some additions notably the strontium and zinc which are in Cornwall Stone but not in Digitalfire's recipe for Cornwall Stone Substitute. I have found the small amount of zinc to be fairly essential in recreating the look of original Cornwall Stone.
I have subsequently replaced the small amount of soda ash and pearl ash with 2% Minspar-200 Soda Feldspar, while reducing the Silica from 26 to 25 and the English Kaolin from 12 to 11. New Improved "chemically identical' now without soluble ingredients.
Please feel free to work on this recipe to find a way to reduce the number of ingredients while maintaining the chemically identical status.
Tenmoku Gold Norm's w/o Cornwall Stone ^6 is my renamed "final adaption" we use at our studio, which is not at all "chemically identical" to the original V's Tenmoku Gold.
I suspect my final adaptation could also be simplified somewhat while maintaining the original chemistry.
An obvious place to start is replacing the Wollastonite with more of the Calcium Carbonate and Silica. 3% Wollastonite is probably too small to affect the melting properties much. Or you go in the other direction with more Wollastonite and less Silica, eliminating the Calcium Carbonate aka whiting.
The recipe was spelled in John's book, Temmoku , two m's. and not with an "n". Both spellings are in data base.
The glaze with the Cornwall Stone replacement does not mention the original glaze before the substitution so I'm not sure if its the glaze I was looking at named Temmoku Gold.
So hard to figure out. I guess if I want to use them I just have to mix some up and test. Glad to have so many to choose from!
I did not see the recipe for V.C. Soft Satin Glossy 1 in the data base.
speaking of Cornwall stone, I saw two glazes in John Britts book last night containing Cornwall Stone, and had to look it up.... Glaze names are Temmoku Gold and V.C. Soft Satin Glossy 1 , both with Cornwall Stone.
Temmoku Gold recipe: Cornwall Stone 67.4, Whiting 9, Silica 6.2, Dolomite 7.9, Gerstley Borate 3.4, Lithium Carbonate 6.2, Red Iron Oxide 11.2, Bentonite 2.
V.C. Soft Satin Glossy 1: Cornwall stone 46, Wollastonite 10, Kaolin 10, Dolomite 12, Frit 3124 8, Gerstley Borate 14, Zircopax 14, Bentonite 2.
Is the Temmoku Gold recipe with Cornwall Stone replacement in our data base?
Any idea what the V.C Soft Satin Glossy 1 recipe would be with a replacement?
I'm not savy with the In -Sight glaze cal. program we use, but hope to get on board for the interactive Webinar , Thursday , March 5.
the cornwall stone replacement glaze.
Did you use Cornwall Stone for the Tenmoku Gold recipe, or the Cornwall Stone replacement recipe?
sorry, just saw where you said, tenmoku gold.
j
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2026 Created by Andrea Wolf.
Powered by
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics