Underglaze and best clear on the body, pearson's bronze on the top and bottom.

Views: 177

Albums: 2013

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Norm Stuart on July 19, 2013 at 12:19pm

Interesting. Some of the nicest ceramic pieces have seen had glazes applied and fired 8, 12 or 16 times. We have a book someplace with a lot of examples like this.  I'll post the title if I find it.

My nephew's Aztec Gold on his Mickey Mouse came out very mirror-like because he applied it to a perfectly smooth previously fired ^6 surface.

After seeing my results of the Spectrum 1116 Metallic Mirror I can see a perfect surface it the key to the final look. The smooth side of the tile is a perfect mirror, but the textured side has some mirrored areas with most being dark glass with a slight green cast to it


Stars
Comment by Kathy Ransom on July 19, 2013 at 8:40am

Just wanted to add though that I brush this glaze on as you mix it up very thick so the only way to apply is with brushing.  Very high in manganese so I don't think I'd want to try spraying it and it is absolutely non-food safe!


Stars
Comment by Kathy Ransom on July 19, 2013 at 8:38am

Thanks Norm but I had to apply and fire, reapply and refire! The first coat peeled a bit and left gaps so I re-applied all over and got a smooth coat the 2nd time around.  This is the first time I've had problems with this glaze peeling so next time I mix it I'm going to try calcining some of the clay. 


Stars
Comment by Norm Stuart on July 18, 2013 at 6:33pm

Kathy - You have quite a deft touch with this glaze on your piece.

This is the Colin Pearson Bronze on a test tile in our kiln with slow-cool between 1800 F and 1500 F.


Stars
Comment by Norm Stuart on July 2, 2013 at 11:53pm

That is a very nice metallic copper Kathy.  I'll have to try it out.

Colin Pearson Bronze ^5/6

100 Manganese Dioxide
  10 Copper Oxide
  10 China Clay


Stars
Comment by Kathy Ransom on July 2, 2013 at 9:32pm

Pearson's bronze is a glaze I make up and one of my favourites!  I can't put my hands on the recipe right now but if you'd like it I will see if I can find it.  This jar is one of my best ones yet and quite large at 15" high.


Stars
Comment by Denice E. Demuth on July 2, 2013 at 8:14pm

Is Pearson's bronze glaze one you make or is it purchased?  This jar is truly elegant.    Denice

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service