Cone 6 Oil can pots. Floating Red Glaze but sprayed on lightly and perhaps a little underfired (did not hold at Cone 6). I was expecting them to come out a little dryer to achieve a rusty look, but exceeded my expectations. They even feel rusty.

Views: 113

Albums: Cone 6

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Jan Wallace on February 28, 2012 at 9:45pm

Thank you Kathy and Sally. I am amazed by the variations we can achieve from the one glaze simply by different approaches to application, firing etc. Hope you had a productive day in the studio. Louis, I had a look at Tim See's website. I Love his work. I had never heard of a 'steampunk' before, so was also educational LOL.


Stars
Comment by Kathy Ransom on February 28, 2012 at 3:17pm
I love your oil can pots! You really got a rusted look with your glaze from spraying lightly. I've spenyT most of my day brushing glazes on because I wanted a particular effect but after coffee I'm going to spray the remainder of the bisque I have on hand in a fraction of the time. Of course it takes 3 times as long to prepare, then clean up!

Stars
Comment by Jan Wallace on February 28, 2012 at 1:02pm

Thanks everyone. I will take some better photos and one with closer detail of the glaze. It's a rainy day here today, so I will get onto that today whilst stuck indoors. I have used the 'Floating Red' glaze before but achieved a very different result (see my photo gallery) on a couple of small teapots. One which looks a little like an oil can as George's comments state under the pic. I used the glaze again as I liked the fact that this glaze gave me a variegated, rusty look despite being a little shiny. BUT, this time by 'happy accident' i sprayed a lighter coat of glaze and as I said before, perhaps a cooler top temp (no soak at cone 6), made a VERY matt/dry rusty glaze. Hope I can achieve this again. I just love it when things turn out well with pieces that we spend alot of time and thought on. So many times with this craft, I am quietly dissapointed. I still have so much to learn with glazing as its all fairly new to me even though I have been potting for years. That is how we learn the most though, isn't it. Louis, I will have a look at Tim's work. Sounds  very interesting.  Denise, the shed they are photographed in front of, is my studio. There are photos in my photo gallery. My husband and I built it from alot of recycled building material to look like an old shed. Inside, the rear wall is made from an old rusting corrugated iron which came from an shed in our local area so has history as well which I love. Its the favourite part of my studio.


Stars
Comment by Denice E. Demuth on February 28, 2012 at 6:52am

Great effect they look like a bunch of old oil cans rusting away outside of a garden shed.   Denice


Stars
Comment by Louis Ford on February 28, 2012 at 4:40am

GREAT work!.....can you show a more detailed photo of the finish?  There is an artist (Tim See) that you should check out...he make steam punks and oil cans of a similar nature.


Stars
Comment by Carl Ray Crutchfield on February 28, 2012 at 4:39am

Very nice work, they make a great display together.


Stars
Comment by Jan Wallace on February 27, 2012 at 10:45pm
Thanks George, they are very addictive. I want to make MORE!!! lol
Comment by George Lewter on February 27, 2012 at 8:14pm

These are great, Jan. Congratulations!

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service